    Default Power Plasma 50 Air Filter Bracket

    It is my understanding that the air filter bracket supplied by Everlast does not give enough clearance on the back of the machine. What have you guys done to fix this? My thought is to put some washers in there to act as a spacer. If all else fails, I will make a new bracket. If you have made a new bracket, please post a pic.
    Hobart Handler 187
    Thermal Arc 161S
    Everlast Power Plasma 50

  2. #2

    Default

    Here you go. Aluminum angle.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Welder-Plasma_04 (Large).JPG 
Views:	417 
Size:	138.3 KB 
ID:	2301  
    Everlast PowerArc 300
    Everlast PowerArc 200
    Everlast PowerPlasma 70
    Hobart Handler 125 EZ
    Lincoln Tombstone AC
    Lincoln Tombstone AC/DC
    O/A outfit
    Honda 11K generator

  3. #3

    Default

    Thanks GWD. How did you attach the angle to the filter? BTW, I like the elbow idea.
    Hobart Handler 187
    Thermal Arc 161S
    Everlast Power Plasma 50

  4. #4

    Default

    Quote Originally Posted by morgaj1 View Post
    Thanks GWD. How did you attach the angle to the filter? BTW, I like the elbow idea.
    The stock bracket was used to determine where the holes should go. The holes on the filter are slightly recessed in the housing so a couple of small triangles were cut from the bracket with a hacksaw. That allowed the filters "shoulders" to fit in the triangles. A better photo may be coming if time permits.

    (Actually, in looking at the photo again, the outward side of the filter is just like the inward side. You can see where the little triangles need to be cut to clear those "flying buttresses", or whatever you want to call them, that are just outside the holes on both edges.)

    The elbow on the filter keeps the hose's quick connect from applying too much torque to the filter/bracket. You likely figured that out yourself.
    Last edited by GWD; 06-09-2011 at 02:15 AM.

  5. #5
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Mine is a PowerUltra 205P and it blocked the CNC port so I made a quick and dirty bracket from a piece of c purlin and attached it to the wall then ran a long hose to the cutter. When I get my cart built I plan to mount it on the cart not the machine.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  6. #6

    Default

    Quote Originally Posted by GWD View Post
    Here you go. Aluminum angle.
    I stole your idea and used 1" alum angle and a elbow. Works great. It is frustrating to have to do this on a brand new unit...
    Hobart Handler 187
    Thermal Arc 161S
    Everlast Power Plasma 50

  7. #7

    Default

    Resolving this on the factory side is a complicated issue, as the supplier of the filter would be the source of the problem and they produce mass quantities and must get through their current stock before they will make changes. A few washers usually take care of any issues.

Similar Threads

  1. HF Filter pressure drop
    By Odyknuck in forum Everlast Plasma Cutters (PAC)
    Replies: 15
    Last Post: 12-17-2012, 03:22 PM
  2. Cast Aluminum Repair on Lathe Bracket W/ Power Tig Micro 185
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 10-20-2012, 05:15 PM
  3. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  4. Replies: 5
    Last Post: 06-18-2011, 08:14 PM
  5. Filter on your 250?
    By Nikola Tesla in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 03-24-2011, 06:19 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •