Share
Results 1 to 15 of 15

Thread: Project 1 from ScratchStart

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Project 1 from ScratchStart

    The DOT was not very happy when my crane lacked the necessary "safety equipment". Which in this case were the 3 small red lights that mark center rear of the vehicle. so I had to build a little light bar and wire some up.

    bar is 2x4x 1/8 square tube. I cut 3, 2 3/8" holes with the plasma (hole saw was MIA) and ground them out to round, as my plasma skills were seriously inhibited by the ammount of coffe I had.


    Cut caps for the end from some 1/8" x 2" HR flat stock and welded them on

    ground the welds down and smoothed them out


    here is the light bar ready for some primer


    The whole project took less than 2 hours (not including time for the paint to dry). All the steel came from the scrap pile.

    I'll grab a picture of it installed and add it.
    Last edited by ScratchStart; 06-06-2011 at 07:52 PM.
    I'd like to think I'm the guy they are talkin about when they say, "he could F%^& up a cannon ball in a plowed field."
    .................. /...\
    ..............-...|.....|
    ...*.......-'. \..\__/
    ....\.-'.........\
    ... /......... _/
    ...|......... /"
    ...|.... /_\'
    ....\....\_/
    ......""""