Share
Results 1 to 2 of 2

Thread: 250 ex 250 amps ac

  1. Default 250 ex 250 amps ac

    had a job for an aluminum transom mount angle is 3/8 thick and the flat bar is 5/8 thick i used the 250 ex with 250 amps and 200 htz 20% dcen 1/8 4043 1/8 arc time tungsten
    i know its not welded solid but its going to be through bolted the customer just want the rigidity of it being welded and having a gusset plate on it.i love this becuase it tested both the cooler that just bought and the wp 20 tig torch setup that i just put together.
    the 250 ex never flinched i had it on for about 3 hours it performed flawlessly and the coolerdid an excellent job i do have a question about it is an itw or bernard style cooler with a procon vane pump it sounds like it there a real low chirp coming form the pump when its in use didnt know if thats normal or not. and also the wp 20 never got above warm during the entire time of doing this job the foot pedal was pretty much smashed unless near an edge.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	0706112221a.jpg 
Views:	506 
Size:	140.0 KB 
ID:	2719   Click image for larger version. 

Name:	0706112221c.jpg 
Views:	503 
Size:	128.3 KB 
ID:	2718   Click image for larger version. 

Name:	0706112221.jpg 
Views:	490 
Size:	136.0 KB 
ID:	2720   Click image for larger version. 

Name:	0706112221b.jpg 
Views:	455 
Size:	146.1 KB 
ID:	2721   Click image for larger version. 

Name:	0706112220.jpg 
Views:	492 
Size:	141.0 KB 
ID:	2722  

    Click image for larger version. 

Name:	0706112219a.jpg 
Views:	489 
Size:	140.8 KB 
ID:	2723   Click image for larger version. 

Name:	0706112219.jpg 
Views:	531 
Size:	140.4 KB 
ID:	2724  
    Last edited by jdt1986; 07-07-2011 at 04:08 AM.

  2. Default

    yet another job with the 250 ex : had to weld in a tunnel on a weldbuld boat had about 3-4 hours of welding with the ex never failed me, going strong . i love this tig machine

Similar Threads

  1. Surge amps
    By Chevelle69 in forum General Welder Questions
    Replies: 2
    Last Post: 02-17-2015, 07:44 PM
  2. Low Amps and HF
    By brianscott in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 02-12-2012, 04:45 PM
  3. amps req. for .095 aluminum
    By backhoe in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 12-05-2011, 04:39 PM
  4. PT 250 EX stuck at 478 Amps!!!
    By Jetfire3 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 06-10-2011, 03:33 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •