Share
Results 1 to 19 of 19

Thread: Press brake for modified HF shop press

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Press brake for modified HF shop press

    I found lots pictures on line of different style press brakes so I thought I would make one too. The dies are 15" wide, the bottom is made from 1/2" plate with three pieces of 2x2x1/4" angle for the bottom die, the top plate is 3/4" X 4" flat bar that I ground a 60 degree angle on. I also added support under the base plate.
    Attachment 1922Attachment 1921Attachment 1920Attachment 1919

  2. #2

    Default

    Here are some pictures of the brake sitting on the press

    Attachment 1923Attachment 1924Attachment 1925Attachment 1926

  3. #3

    Default

    The first time I used the brake I decided it needed a small outlet table with a movable guide to keep the bends square, so this is what I came up with.
    Scooter

    Attachment 1928Attachment 1927Attachment 1929

  4. #4

    Default

    Scooter, I have been thinking of that guide strip to keep it at 90 degrees, make a mark on it and then you could use it to reference your bend point, say the bend is like at 3 inches on the metal and the mark is 2 more inches, so all 3 inch bends get marked at 5 inches, you wouldn't need a back stop that way. An idea anyhow.

  5. #5

    Default

    Scooter.

    Did you plasma cut then grind, or all grinding on the 3/4" top plate ? What made you go with 60 degrees? Read somewhere 80 is the magic number for 90 bend. Where you going for more than 90? HF has a 20 ton on sale for $169 again and it keeps getting my eye. Though I have some "I" beams I can cut up and the jack is like $50..
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6

    Default

    Mike, I did not have the plasma cutter when I did this, I put a new disc on the 9" Milwaukee grinder, laid it flat at the angle I needed and just kept going back and forth, then finished it off with a big file. I used 60 degrees because thats what most people were using when I read about press breaks. I bent some 1/4" and it will bend a little more than 90 degrees, I was not sure how much the work piece would spring back if any? I plan on getting a 20 ton air over hyd jack for it someday. I probably should have just built the press after everything I did to it?

  7. #7

    Default

    Quote Originally Posted by geezer View Post
    Scooter, I have been thinking of that guide strip to keep it at 90 degrees, make a mark on it and then you could use it to reference your bend point, say the bend is like at 3 inches on the metal and the mark is 2 more inches, so all 3 inch bends get marked at 5 inches, you wouldn't need a back stop that way. An idea anyhow.
    Geezer, good idea, mind if I borrow it?

  8. #8

    Default

    Thanks Ken, I have only bent one piece so far and then I added the outlet table and have not used it since? I have been building stuff for the last couple of weeks that I sketched up over the winter. Most of it has just been upgrading my tools. The next project is a set of equipment style ramps for the trailer.

  9. #9

    Default

    Very nice work Scooter, I like your use of plug welds, that's something I use quite a bit myself. question,,,where did you get those nice springs. I haven't done much on my own build, been too busy on other things, I stole /borrowed some idea's from Ram48 and I can see some idea's on your build that I would like to use.
    Like the guide to keep the bend square, that's a smart feature.

  10. #10

    Default

    Thanks Geezer, I got the springs at Tractor Supply they have all different sizes and they are normally on the end of an isle back by the chain and cable area.

  11. Default

    Very creative idea for the bottom die. I'm impressed! What has been the maximum tonnage it's been put under, and how is it holding up? I guess my concern is what happens if the welds fail at high pressure and the work piece or pieces of the die escapes at high velocity. Just wondering.

    FYI: Two more sources for all things "springy" McMaster Carr at http://www.mcmaster.com/, and Reid Supply at http://www.reidsupply.com/
    David Shearer
    Machine Shop Services
    Arroyo Grande, CA
    davidshearer1956@gmail.com

  12. #12

    Default

    Thanks David for the info, as far as a velocity concern on failure, I don't see that as much of an issue, failure would most likely involve some creaking, bending and a possible bang, but no serious movement, similar to concrete cylinder breaking or elongation testing for bolts or wire, a bang and some movement but no flying debris.

  13. #13

    Default

    David, like Geezer said I don't think there is much of a chance of the brake coming apart, I would never try to bend any type of hardened steel so the work piece won't be a problem either. With only a 20 ton jack the worst thing that will happen is the jack will run out of force and stop.

Similar Threads

  1. Custom 30 Ton Press Modification
    By cbmkr in forum Personal Projects (no welder required)
    Replies: 13
    Last Post: 09-27-2013, 09:30 PM
  2. Project 1 by redbeard : Hydrualic Shop Press
    By redbeard in forum Other Custom Fabrications
    Replies: 12
    Last Post: 11-10-2011, 07:55 AM
  3. Press for the brake. $35 total, that was for the jack.
    By chadford in forum Other Custom Fabrications
    Replies: 10
    Last Post: 07-19-2011, 12:17 PM
  4. Press brake
    By Ram48 in forum Other Custom Fabrications
    Replies: 34
    Last Post: 03-28-2011, 03:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •