thanks for the positive comments, guys. the short lead on the gun gave me the idea to put the holder up high. it saves me from having to coil it around a peg or something similar.

the drawer is nice, but I think I made it somewhat obsolete by adding the 6-drawer cabinet. the big drawer is nice for gloves, but in hind sight, I'd probably do 2 smaller drawers for gloves rather than a big one. it did take a while to square everything up and get the drawer going. I think that took longer (probably 2.5 hrs) than any other single thing. but, then again, had I thrown caution to the wind and welded it in, it would've taken about 45 minutes. drilling holes sucks.

the rest of the pics:
I thought I had a good shot of the top shelf. I forgot to take pics until after I had already turned the big high pressure sodium lights off, so they're all a bit dark.

a little better view of the bottom compartment. the opening is 11" high, sized around the sawzall case. I dunno the size of the everlast water cooler, hopefully it fits, if not, I can manage to make my own. I suspect the sawzall will get kicked out when I get a cooler.

I believe the inside dimensions of the tray are 19.5x25x13"
the bottom frame is 2x2x1/8" and is the only thing that isn't 1x1x1/8" angle, save the gun holders.
Attachment 2061

this is a hat hook I made for my dad's tig. he has a nice speedglas with the respirator that he keeps in a big tupperware box. I got tired of hanging my hat on the tank valve. I think I made the band out of 20ga with the edges rolled over. the rod is, I think, 3/16" hardware store rod bent in the vise. I've lost the bolt, but it's threaded for a 2" 5/16"-18 bolt. it's a pain to get in there because I didn't drill the non-threaded hole big enough to let the bolt wiggle when you're bolting it together. should've used an oversized hole and a washer.

anyway, it's a good coat hook, too. unfortunately my 48" split leg apron (which on my short arse goes to my ankles) is too long to hang from, so it gets draped behind the bottles.

the other photo is just a better shot of the magnetic tig torch holder.
Attachment 2062Attachment 2060

I'll try to take some better pics of the top shelf tomorrow.