UPDATE: Replaced the 4053 chip and diode along with adding in the cap and all is well again. Then I had an odd problem where the arc would jump when the pedal was halfway down. Turned out to be a dead spot in the POT that's in the pedal itself. Replaced it and it's working great. Now just waiting till the 20 series torch comes in to try that little beast out.