The Everlast MIG torch WP-18 nozzle is removed by pulling it straight off, you can rock them if needed.
If you attempt to unscrew the nozzle, it's possible you could damage the retaining spring that holds the nozzle on.
The nozzles can be purchased at your local welding supply, but I am not sure if the spring would be a normally stocked item.