ok I see 1300 is not ruuning out...down to 1100 now...bumping the flow up tp 15cph did the trick on aluminum so far, and getting nice beads
ok I see 1300 is not ruuning out...down to 1100 now...bumping the flow up tp 15cph did the trick on aluminum so far, and getting nice beads
sold my miller mig
got a PT250EX
saving up for a plasma cutter
Your regulator should be seeing about 45 psi when it's flowing. SO use the tank until it's all the way gone. No sense in wasting some of that gas before ya gotta
ok will do - and here I was ready to take it back at 1000psi
sold my miller mig
got a PT250EX
saving up for a plasma cutter
____
Ray
Everlast Sales and Support Team.
support@everlastalaska.com
www.everlastalaska.com
877-755-9353 X207
Just weld away till it's empty. How big of tank is it?
330cf - been running the 250 quite a bit since I got it
sold my miller mig
got a PT250EX
saving up for a plasma cutter
Well I didnt want to get stuck over the weekend with no gas, I took it down to a little under 100psi and took it in for an exchange. The refill was 4$ less this time, glad I got the 330 rather then a smaller tank
sold my miller mig
got a PT250EX
saving up for a plasma cutter