    Ok If their is any interest I can take some pictures and let you figure it out from there as I made no drawings and did this right when I started welding again after like 20 or so years off, maybe 3 years ago.

    what I did was make a pivot arm for a Harbor Freight hand held portable band saw. The cost of the band saw on sale and with a 20% off coupon was about $59 and I figure another $10 in material.

    Materials were all scrap from other projects. some 3/16 as a base to bolt to work table, 2 small 1/2 plate rems about 5x5", a piece of 10" long 1/2x1" bar and a 4" piece of angle iron.

    If there is any interest in seeing pictures or a video of it in action I will post up some pictures and a video like to youtube ( I'll have to shoot the video)

    I figure like a lot of you my budget had no room in it for a big horizontal band saw and I hate how long and loud a chop saw takes to go though 2" .250 wall square tube or anything up to 4" ( the opening of the saw ). with a good 10-14 bi-metal blade this thing makes short work of .250 wall tubing or anything up to 4"x4" and that could be solid .

    The blades I bought were also from HF but were amreican made. Morse Bimetal 3 blades for $19 but starret and other good blade companies make bimetal blades for this saw because Milwaukee and other make a similar saw with the same blade size Except the others cost about $300 or more.

    the cuts are dead straight too ( god only knows why ) as I figured I just wanted to get the cuts fairly close but the cut end of square tube will stand up dead straight on a flat surface with a square on 2 90 deg apart sides.

    Its ugly as hell but works great and only takes about a couple hours and cuts about 10 times faster than a chop saw without all the noise and sparks & mess. any interest let me know.
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  2. Default

    Those things are $200+ on ebay. the vertical one is $72 plus shipping.

    Post pics.

    You can order just the swing arm on ebay for about $53.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  3. #3
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I am totally interested. Post pics and details!

    Although I just bought a bandsaw, its a bit of a "basket case" so I can use all the info on them I can get. Also, I'd like to see how you make one custom!

    I feel like I got a deal on the one I got, its a vintage "craftsman industrial" (made by atlas / clausing) horizontal 3x6 I bought for $40. I've already sunk about $30 of additional in parts into it and am not done yet. But it has neat features... a hydraulic cylinder, pretty decent construction. A real nice homemade stand. Nice, lightning-quick starting 1/2 hp motor. Maybe I will start a thread on its restoration and review myself if there is much interest!

    So far I already have it up and running, and really like the utility of these horizontal metal cutting bandsaws. So much quicker and more accurate than hacksawing... By the way, I put a 24 tooth per inch high-carbon blade, and am finding I can cut things thinner than I ever could with a hacksaw... I'm talking thin (and fragile), .020" thick aluminum extrusions stood up on end, cut sideways through the wall, without causing any wall distortion.
    Last edited by jakeru; 05-07-2011 at 12:50 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. Default

    http://cgi.ebay.com/Milwaukee-48-08-...item5adfb3d4a0

    http://cgi.ebay.com/Stout-ST-CS250-p...item19c515333d

    http://cgi.ebay.com/ws/eBayISAPI.dll...=STRK:MEWAX:IT

    Does anyone here have a STOUT brand portasaw? I'm willing to buy one just to get the table saw attachment.
    Last edited by ducksface; 05-07-2011 at 01:15 AM.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  5. #5

    Default

    I'm going to be laid-up for a while unfortunatly but will get my Dad to get a few pics, I'm pretty depressed right now, just discovered I have a pressure sore under my left hip on my left buttock which means about 6 wks of mostly in bed. guess I been up in my wheelchair too much lately.

    But basically what I did is make a pivoting arm for the band saw that allows me to cut heavy steel with little effort, noise or mess. I will get the pictures up asap for ya and possibly I can get my dad to make some cuts on some material for a video also.

    This is basically my life... just when things get going on an up note for me I get a sore or some thing happens to put me in the hospital or out of commission for a month or 2 .
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  6. #6
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Definitely take care of yourself, and keep your chin up. The metal can wait.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  7. #7
    Join Date
    Jul 2010
    Location
    Lloydminster, Alberta Canada
    Posts
    28

    Default

    All the best Don.


    Chuck

  8. #8

    Default

    I'm going over to my Mom's today after my Dr visit , will get some pictures while there for ya guys . Possibly some video too. I just have to limit my sitting time and try to keep most of the pressure on my other hip.

    The sore is not very big 1cm x 2 cm it could easily get infected and much larger very easily so I gotta take it easy.
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  9. Default

    There's a used factory Milwaukee one for sale on ebay. I bid $100 for the frame, it's going to sell for way more than that. I'll be building yours instead.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

Similar Threads

  1. Portable Horizontal Bandsaw
    By zedron in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 7
    Last Post: 08-10-2013, 12:33 AM
  2. Project #5 Home Made Scrolling Wrench
    By Powertig in forum Hobyist Projects
    Replies: 10
    Last Post: 02-20-2012, 03:33 PM
  3. Home made cable covers
    By Tom C in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 01-20-2012, 04:45 PM
  4. Aluminum sheetmetal shroud for under-mounted Horizontal Bandsaw motor
    By jakeru in forum Other Custom Fabrications
    Replies: 2
    Last Post: 05-08-2011, 05:07 PM
  5. Home made rotisserie
    By Jason in forum Other Custom Fabrications
    Replies: 11
    Last Post: 03-21-2011, 01:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •