    Default low amperage stick welding with PU 205

    I haven't used the stick weld function on my 205 much at all, bought it for the TIG , the Plasma and the portability.

    I have quite a bit of stick welding to do for a customer out on a jobsite. The plan is to use the little Everlast rather than lug my 500 lb Miller/Onan over there and listen to it roar.

    This job is for a customer I first worked for in 1988. My Brother and I built an Architect designed house for him. The house had all kinds of wide flange beams and 4x4 steel posts, so there was quite a bit of steel fab work for to do. We decided to pack the welder into the basement area so that the welding cable length would not be too great. It got chained it to a post and left on the job for about a month and was used an hour or two every day.
    The owner and two of our carpenters helped me pack the beast in.

    This time around, he is building another Architect design home with steel work, but someone else is doing the building. He asked if I would do the structural steel part , which I am happy to do.

    It will be interesting to see his expression when I walk in with this little green box under my arm!

    Today I tried welding some scrap bits of .065SS in stick mode. I won't be switching over from TIGing this type of weld, that is still the nicest way to go, but I thought it did an OK job on the thin wall material. I have done welds of this type in the past with the transformer welders. They didn't turn out quite as good, the arc always kept going out. I had no problem with that today however. I guess that is the inverter advantage.

    This was done at about 35 amps.

    Tomorrow I might pick up some 7018 and try welding some 3/16" to 3/8" wall mild steel scraps. 3/8" is the thickest material I'll encounter on this job.

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  2. #2

    Default

    You can do a lot of things with stick, my PA 200 is sure an improvement over an old Thunderbolt and a home made DC rectifier unit. You should have no trouble doing 3/16 to 3/8 wall with 7018 using a 1/8 rod. I guess I will always be a stick guy. Have fun, sounds like you are really getting you moneys worth out of your unit.

  3. #3

    Default

    I love stick welding myself, it's what I prefer to weld with. Mig welding is handy, quick, and good for production. Stick welding takes a little more time to learn the rods and how to run them, but you can run just as good of a bead with a stick welder.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. 200 dx welding stick problems
    By steve1989 in forum General Welding Questions
    Replies: 2
    Last Post: 03-02-2014, 04:42 PM
  2. Stick welding aluminum?
    By undercut in forum General Welder Questions
    Replies: 14
    Last Post: 05-13-2012, 11:48 AM
  3. Preheating to help Stick Welding
    By undercut in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 05-07-2012, 07:30 PM
  4. Stick welding questions:
    By I_Love_Plasma in forum Stick Welding (SMAW)
    Replies: 30
    Last Post: 02-15-2012, 05:09 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •