    Default Aluminum TIG fin building. Anyone tried it??

    So, before I got the crap scared out of me yesterday(see the thread on heart trouble). I decided to play around with different cup sizes, filler materials, Lanthanated vs. tungsten, etc. I have an old piece of cast aluminum that I have been using to bone up on this stuff. Decided to see what would happen if I just laid one bead on top of another. Here's what I got.




    This will really come in handy on the old bike parts that I've mentioned before where there may be a piece of casting broken away. I'm thinking that next I'll sand the sides of the fin smooth and fill in the imperfections to make it into a perfect "repair"
    I was using my old Linde with 3/32" tungsten alternating between 1.5% lanth and 2% Thoriated. I honestly think I prefer the Lanthanated. Even though I'm running an old transforner machine, I sharpen to a point and let the electrode do what it's going to do. After 2 or 3 passes the Lanth tip formed a ball about 1/32 inch. Arc was relatively controllable, and actually got better by switching from a #5 to #6 cup. 17cfh on my flowmeter, Weldcraft WP20 torch (water-cooled). I was at 180 amps and had my pedal about 3/4 of the way down most of the time. A little more if the oxide layer covered the puddle, a little less if the puddle looked like it was going to collapse. I recomend this as a good way to learn how to develop judgement on how much pedal to use.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  2. #2

    Default

    You have a pacemaker?

  3. #3
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    Hey Mark, please see new thread "can welding affect your heart?" I need answers.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  4. #4
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    That's a pretty extreme build-up! Nice work, definitely takes some patience to pull off.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  5. Default

    Hmmmm, That reminded me of a cracked primary cover for the harley. Never had the heart to throw it away since it was originally bare casting and I put a lot of work into it hand polishing it and had it chromed.
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

Similar Threads

  1. Building of a forged mirror
    By donor76 in forum Metal Art
    Replies: 5
    Last Post: 01-22-2015, 11:23 PM
  2. Building a burner for a gas grill
    By trickbiker in forum General Welding Questions
    Replies: 5
    Last Post: 09-01-2012, 04:20 AM
  3. building a raised deck
    By dgarnier in forum General Welding Questions
    Replies: 8
    Last Post: 07-27-2011, 12:03 AM
  4. pictures of the car I am building
    By Wrenchtamer in forum Other Custom Fabrications
    Replies: 5
    Last Post: 06-06-2011, 11:16 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •