Well, this project isn't really by choice, but I will need to fab a new turbo header for my bike. Did some tuning on the dyno this weekend, hoping to get up near or over the 500HP mark and got stopped short from a broken header.
Only made it to 361 rwhp before I had to stop when the turbo literally removed itself from my header.
It was quite hot a few times throughout testing with the load cell, although the picture below makes it look a bit hotter than it actually was (camera adjusted to the dark room and may have picked up some of the infrared from the header).
New header will consist of an investment case 304 one piece flange and head spigots and schedule 10 304 stainless weld els. I will probably weld it with 308L and 2% Lanthanated tungsten.
John
![]()