    Default 200dx Stick Welding Questions

    Can I run a 6010?

    How many feet of welding cable can I use, the stock leads are short and I would like to add some length. What would be to long?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2

    Default

    Sean, I think 6011 would be your best bet, although I have not tried that machine so it may run 6010 as well. As far as cables go if they are big enough they can go on for ever, well almost for ever. I think the last time I extended them I used one size bigger cable and added 15 or 16 feet, that plus the original cables gives me pretty good reach, You are about to learn how expensive copper wire is, it's an eye opener , believe me.

  3. #3

    Default

    Its not designed for 6010, though you may be able to get it to run at higher amps, but control won't be as well. Geezer is right about using 6011, it will run better.

    I would not go over 50 ft, though that isn't necessarily the limit. We have customers using the PowerArcs with some pretty long set ups. The longer the cable, the heavier the gauge. I'd go with #2 or bigger for best results.

  4. #4

    Default

    Thanks guys, I have not used my machine as much as I would like, been busy. I'm lining up a couple projects for the weekend and wanted to know before I tried.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5

    Default

    6011, 7014, 6013, and fresh 7018's are all good rods for the unit.

  6. #6

    Default

    I broke out my machine and did a little stick welding today, I am impressed with all the power and how good of a job it will do. It has plenty of power for my needs.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. New 200dx owner with a few questions
    By Toby in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 12-14-2012, 02:21 AM
  2. New 200DX questions
    By Bigwilly01 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 07-19-2012, 02:35 AM
  3. Stick welding questions:
    By I_Love_Plasma in forum Stick Welding (SMAW)
    Replies: 30
    Last Post: 02-15-2012, 05:09 AM
  4. 200dx questions
    By budracer1 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 02-07-2012, 05:55 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •