Share
Results 1 to 3 of 3

Thread: My favorite settings for various cuts, metals and thickness

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Lightbulb My favorite settings for various cuts, metals and thickness

    How about a post of settings you use for various things, in an intelligible format such as;

    Plasma or TIG
    Metal type
    Flat or inside corner or outside corner or curve
    thickness
    argon flow or alternate gas
    pulse settings ac or dc or reverse
    Pre flow post flow
    upslope down slope
    2t/4t

    Some sort of setting for each dial


    Some person better at this than me can make a quick format to use so we can easily get a good crack at saya s common as...an aluminum butt-weld. Or as obscure as a Magnesium pipe weld. There is lots of information to glean from the posts already here, but a 'favorite settings thread would be very very nice.

    The settings can be used as a starting point as your mileage may vary, but it IS a starting point, and all in one thread.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  2. #2

    Default

    Jody (welding tips and tricks) touches on a few of these for the PP256, can't remember which video tho... I'll watch em and post up some quotes.

    But his vid. on the PP256 is the reason I NEED one... may have to trade my wife for one. Wonder what Robert Redford is doing this weekend....
    I'd like to think I'm the guy they are talkin about when they say, "he could F%^& up a cannon ball in a plowed field."
    .................. /...\
    ..............-...|.....|
    ...*.......-'. \..\__/
    ....\.-'.........\
    ... /......... _/
    ...|......... /"
    ...|.... /_\'
    ....\....\_/
    ......""""

  3. #3

    Default

    75amp
    ac
    90% balance
    1/16th tungsten is NOT a good setting unless you need to shorten the tungsten
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

Similar Threads

  1. 210 EXT Welding Capacity (thickness)
    By MoparCar in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 08-13-2012, 08:42 AM
  2. Powertig 185 cannot melt metals
    By judy in forum General Welder Questions
    Replies: 10
    Last Post: 05-19-2012, 04:33 PM
  3. Help with metal thickness and fit...
    By CGCINC in forum General Welding Questions
    Replies: 9
    Last Post: 12-11-2011, 11:10 PM
  4. Aluminum and Stainless Thickness
    By morgaj1 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 07-04-2011, 05:40 PM
  5. Welding thickness amp settings
    By Mad-Dax in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 09-28-2009, 08:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •