Quote Originally Posted by Scooter View Post
I got to use the new PA200 without the 6010 port today, the thing ran 6010 great no problems at all, I even stuffed it a few times deep into the puddle to see what would happen and it just kept going. I then ran about 5 lbs of 1/8th 7018, old stuff that has been around about 5 years and never in a heater. What works for me is to lay the rod over the vise and heat the bottom half of the rod with a torch to get it dry then it runs fine for me? But the little welder was amazing it ran the 7018 way better than my thunderbolt (old with a dc rectifier attachment). The 7018 restarted very easy with just a little tap on the work piece. I am impressed with the welder. Mark, no need to get me a welder with the 6010 port, I'm good.
Thanks Scooter
Glad to hear you like it, I also had a DC rectifier setup for my thunderbolt built it my self out of some surplus diodes , worked pretty good but not near a good as the PA 200, I'm sure you will be a happy camper with the PA 200 I sure like mine.