So last nite, I was about ready to pull my hair out. I was trying to put spot welds on my tailgate back in, and every time i got a puddle started, it would jump back up the tungsten and form a big goober on the end.Like this.
In order to accomplish 15 or so spot welds, I had to re-sharpen about 10 times.Lucky I had 4 pieces of tungsten available. After I turned the amps up to about 120, I was able to pedal a puddle into the center of the spot, and back off a little to get this result.
Any ideas why I was getting this problem? I can see that I need to resolve this issue or doing panels will be a pain forever. Thanks!