    Default Bar-joist type beam for a loft

    I made this beam for a loft in my shop. It spans 26' 9" and is 12" tall. I built it out of 4 pieces of 1 1/4"x 1 1/4" x 1/8" angle and a piece of 3/8" rod that I bent back and forth at 90 degree angles. I had to splice every piece so that I could get it to the right length. I am not a engineer but I welded it with a 3/4" crown and the way it sets now it still has a 3/8" crown it does not flex it is very solid. Now I have a place to put more stuff!
    Attachment 1513Attachment 1514Attachment 1512
    Power Tig 250 EX
    Miller 211 Mig
    Hobart Stickmate LX
    Victor Torch

  2. #2
    Join Date
    Mar 2011
    Location
    Apache Junction, Az
    Posts
    90

    Default

    I built a similar loft in my shop last week. Mine spans 38' 8" and I made it 10' deep. I considered a joist design like yours, but then I chose to simply put 4 posts under the 2 x 8's.

    I like your open design. I may copy that for my next 2 storage lofts on the sides of the shop. They will be 4' deep by 34' long, so I don't want to use posts as they will interfere with the work tables under them.

    Have you considered adding a couple light fixtures in between the floor joists?
    Hobart Handler 175
    Hobart Iron Man 230 with spool gun
    Thermal Dynamics Cutmaster 52
    Makita Cold Cut Saw

    Possible future addition:
    Lincoln Invertec V311
    or Miller Dynasty 350
    or ???

  3. Default

    looks good
    everlast i-mig 200
    96 gmc extended cab truck 350 rwhp daily driven for 289,000 miles
    88 jeep cherokee custom built by me for me for well everything.someday it'll be finished
    4.6L stroker,dana 44 front, 14 bolt rear, 35"xterrains,soon to come 231/205 doubler

  4. #4
    Join Date
    Feb 2011
    Location
    West Palm Beach Fl.
    Posts
    68

    Default

    Quote Originally Posted by A/C Guy View Post
    I built a similar loft in my shop last week. Mine spans 38' 8" and I made it 10' deep. I considered a joist design like yours, but then I chose to simply put 4 posts under the 2 x 8's.

    I like your open design. I may copy that for my next 2 storage lofts on the sides of the shop. They will be 4' deep by 34' long, so I don't want to use posts as they will interfere with the work tables under them.

    Have you considered adding a couple light fixtures in between the floor joists?
    Yes I have, eventually I will get some light under there, I really need it over the saw so I can see what I am doing. But right now I seem to spend my spare time learning to weld on the new PT250EX. Good luck with your new additional overhead storage area.
    Power Tig 250 EX
    Miller 211 Mig
    Hobart Stickmate LX
    Victor Torch

  5. #5

    Default

    Quote Originally Posted by Salty View Post
    I made this beam for a loft in my shop. It spans 26' 9" and is 12" tall. I built it out of 4 pieces of 1 1/4"x 1 1/4" x 1/8" angle and a piece of 3/8" rod that I bent back and forth at 90 degree angles. I had to splice every piece so that I could get it to the right length. I am not a engineer but I welded it with a 3/4" crown and the way it sets now it still has a 3/8" crown it does not flex it is very solid. Now I have a place to put more stuff!
    Attachment 1513Attachment 1514Attachment 1512
    One thing you need to bare in mind is a joist like this generally have the top chord fully braced by decking, In your case top chord buckling is limited only by how well you attached your ledger - kind of a complicated analysis. Also the bottom chord is not really meant for loading. If you check out the Steel Joist Institute web site you should find some info on loading joists.

  6. #6

    Default

    Quote Originally Posted by sm95m View Post
    One thing you need to bare in mind is a joist like this generally have the top chord fully braced by decking, In your case top chord buckling is limited only by how well you attached your ledger - kind of a complicated analysis. Also the bottom chord is not really meant for loading. If you check out the Steel Joist Institute web site you should find some info on loading joists.
    for Sh*ts and giggles I modeled on the computer with a 50#/ft dead load and a 100#/ft live (storage) load and the 3/8" rod is overstressed as much as 145% - especially at the ends where the web members do most of the work. if you look at a manufactured bar-joist the web members are small but bigger near the supports. heaviest loaded diagonal is the last one on each end. Deflections are OK @ full 150 PLF load
    250 EX
    Miller 211
    Miller 625
    Enco 12X36
    Lathermaster Mill
    and other fabrication and building stuff

  7. #7
    Join Date
    Apr 2011
    Location
    Sasktachewan, Canada
    Posts
    95

    Default

    From what I can see that trust was built for some serious floor loading. That trust looks very similar ones we have in boiler room floors. They support a steel deck with a 4" concrete on top on 24" spacings. I would suspect it can carry a fairly heavy load. My only concern is with the attachments to the wall and the bearing surfaces on each end of the truss. Our building codes (up here) typically require a minimum 3" load bearing surface. I would suspect your building codes will be fairly similar. It appears your bearing those loads on a 1 1/2" bearing surface? I am not sure how the floor joists are attached to the block wall, but blocks are very weak in respect to horizontal loading or pull out resistance. I would be inclined to have these checked before adding any additional weight. I am not criticizing your workmanship simply pointing out possible areas of concern from a structural stand point.
    Attitude Determines Altitude

  8. #8

    Default

    nice job there, you my friend just gave me a great idea for a soon to be travel trailer/carport cover project.
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

Similar Threads

  1. Upcoming project...need some Duct like in a loft???
    By CGCINC in forum General Welding Questions
    Replies: 16
    Last Post: 10-24-2013, 07:52 PM
  2. VW front beam modification
    By youngnstudly in forum On Road Fabrication
    Replies: 0
    Last Post: 08-30-2013, 09:51 AM
  3. Firetruck Loft bed....
    By CGCINC in forum Personal Projects (no welder required)
    Replies: 8
    Last Post: 02-06-2013, 01:04 PM
  4. Heavy duty I beam welding question.
    By Brian Ski in forum General Welding Questions
    Replies: 3
    Last Post: 05-25-2012, 03:27 AM
  5. Project 5 from Worntorn -4 stalls , tack up aisle + Hay loft Barn Addition
    By worntorn in forum Personal Projects (no welder required)
    Replies: 2
    Last Post: 06-12-2011, 10:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •