Ok first Off I started with a set of plans from www.gottrikes.com I'm Building the B version.
1st pic) This is me mooching my neighbors mill LOL self portrait and all these with my Phone.
Attachment 1487
2) the is how the mill started the day off dusty and clean , Muahahah just wait LOL
Attachment 1488
3) Decided to start with the Draw bar construction and the milling and drilling on the 2 18" x 3" x1/4" arms.
Attachment 1489
4) After cutting them to a tad over 18" setting up to skim them down to 18 on the button.
Attachment 1490
5) After Dye chem and some measuring and scribing. I start my Pilot holes, I'm using 2 other drill bits of the same size butt end in the holes to keep the parts aligned while drilling that way I only have to clamp on one side.
Attachment 1491
6) I enlarged the smaller holes from the previous photo to all 1/2", and still using the butt end of one of the 1/2" drills I am boring 7/8" holes now. Some remain 7/8 and one gets enlarged to 1-3/8"
Attachment 1492
7) Final Product two exactly 18" Long, 3" x 1/4" with holes that match exactly because I drilled them stacked and used aligning pins in the holes during every drilling and milling process.
Attachment 1493
That's about it for now I got a bunch of 2" square stock to cut, when I get to more technical or assembly/welding I will continue.... Stay tuned