  1. #1

    Default Size of the cup?

    Attachment 1468So anybody got some easy rules for following the size of the cup? Does it matter if I have an oversized cup on? I bought this half inch cup and so far I like it. I had intended to use it for messing around with titanium. I think its about half inch. Whatever a number 12 is? So I was more curious on wether or not does it matter if you over shoot on the size of your cup? We are talking tig welders here, lol. I attached the cup to show you. The one next to it is the largest that came with the 250. Makes it look tiny.
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  2. #2
    Join Date
    Oct 2010
    Location
    Queensland, Australia
    Posts
    23

    Default

    Frank,

    No harm in going to a larger cup except that it restricts your view a bit and would be harder to get into tight spots. You would probably need to increase the gas flow. I use an oversized one for stainless work.

    Your number 12 cup would be 12/16 of an inch. In other words that cup has a 3/4 inch hole in it.

    Check out the miller site for rules of thumb but what I’ve seen is this:

    Cup size (in 16ths): 3 to 4 times the electrode diameter (so for 1/16 tungsten use a #4, 3/32 tungsten use a #5 or #6 cup, and so on).

    Tungsten sickout: No more than the cup diameter.

    Gas flow: Same litres/min as cup size.

    Post flow: 1 second per 10amps of current.

    Chris
    Brisbane Australia.

  3. #3
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Hi Frank,

    Here is a video using a large size cup for titanium even though the title indicates stainless: http://www.weldingtipsandtricks.com/...stainless.html

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

Similar Threads

  1. i-mig 205 Spool Size
    By MoJo1917 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 9
    Last Post: 09-23-2012, 12:43 PM
  2. Replies: 26
    Last Post: 02-22-2012, 11:25 AM
  3. PowerArc 200 size
    By Scooter in forum Stick Welding (SMAW)
    Replies: 8
    Last Post: 03-04-2011, 09:21 PM
  4. collet size vs tungsten size
    By docweathers in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-08-2011, 03:31 PM
  5. What Mig size for lots of 3/8 & some 1/2
    By geezer in forum General Welder Questions
    Replies: 4
    Last Post: 01-04-2010, 01:02 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •