  1. #10

    Default

    Yes those socket heads do look tidy, don't they?

    Today I used the little multifunction Everlast to plasma cut some 1/2" thick plates needed for mounting the adjuster and for mounting the tool arm, which will be removeable or "modular" as described in the Imperial sales brochure.

    I cut these out of some old material I had on hand. After cutting them I realized they were not quite a match when laid together, so I spent a bit of time with a big cutter on the mill flushing them up.
    This wasn't really necessary but the end product will look a little better for it.

    The photo shows the adjuster welded to one of the plates. A matching plate will be welded to the end of the horizontal upper 3x5 frame member, then the plate on the adjuster will get bolted to that.

    This weld is a fillet between the 1/2" plate and the 1/4" wall adjuster tube. My Miller TIG calculator said this weld should be done at 310 amps. The little Everlast only goes to 200. I was tempted to rig up my old P+H 400 amp, but that requires a bit of effort.

    Feeling a bit lazy, I gave the Everlast a try. How did it do?
    Don't need no stinkin Miller calculator or big honkin welder, just floor the little Green thing and away you go, start melting rod.

    Truth be told this was about max for the unit, but pretty amazing, this is kind of thickness I used to weld when fabbing Caterpillar D6 Clearing blades. Except those were done with a 500 amp Miller 3phase DC stick welder!

    Glen
    Last edited by worntorn; 04-01-2011 at 02:39 AM.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

Similar Threads

  1. Replies: 12
    Last Post: 02-08-2013, 05:17 AM
  2. luvin my Steering wheel
    By azlo in forum On Road Fabrication
    Replies: 5
    Last Post: 12-27-2012, 04:00 AM
  3. english wheel
    By charger891 in forum Other Custom Fabrications
    Replies: 2
    Last Post: 05-09-2012, 01:12 PM
  4. NEW A81 Trafimet Wheel Guide
    By Titan winch in forum Everlast Announcements, Contests and Promotions
    Replies: 0
    Last Post: 07-05-2011, 05:30 PM
  5. added axle to 5th wheel
    By starvingartist in forum Heavy Equipment and Commercial Projects
    Replies: 1
    Last Post: 06-20-2011, 07:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •