Quote Originally Posted by kenwhite View Post
My helmet lets me manually set it to 5 when using my Cut50D. If your helmet won't let you go that low, then a set of safety glasses with 5 tint should work good.
I have some sample helmets that i am seriously considering ( Mark has been evaluating the one style for the last few months ) these have the grinding function and the lower settings 5 is the shade i find best suited for using the plasma as well