get some 1/2 inch to 1 1/4 inch thick steel plate depending on how heavy of stuff you are going to make anything smaller then a 1/2 tends to turn into a bowl after some use and is no longer flat for me a flat surface is important
get some 1/2 inch to 1 1/4 inch thick steel plate depending on how heavy of stuff you are going to make anything smaller then a 1/2 tends to turn into a bowl after some use and is no longer flat for me a flat surface is important
Lincoln precision tig 275
Miller Syncrowave 350 Tig
Miller 250 Mig
old miller 200 Mig
HF 151 Mig
HF 100 FC
Victor Journeyman Oxy/Ace set up