Hi guys,
I bought this unit on February 22nd And received it very quickly on the 28th. Had definite shipping damage right as I opened (regulator broken, foot pedal bent) and upon trying to use the unit it at first would not even make a dent on 16ga aluminum piping. After an hour on the phone with MIke trouble shooting we found that the spark gap had been effected from shipping and I closed it up per his advice. After that it worked pretty good but still had a weird intermittent hiccup where current would be lost. After being roughly 10 minutes off the phone with Mike the gas flow to the gun stopped. Checked the bottle, regulator and lines to the machine and there was sufficient flow. I could hear the relay clicking to initiate the solenoid to open and close but still nothing. This was still using the setting that Mike had me set it to when we were trouble shooting.
I took the air hose and shot air through it to see if the solenoid wasn't opening at all or of it were possibly partially opening, and when I would press the pedal and the relay clicked air would pass through but no where near sufficient amount as this was 65psi that we were applying in short bursts and when welding we run 25-30.
Alex has been more than helpful with this as well as everyone that answers emails. Sent the machine in for warranty repair and Eric said the solenoid is probably jammed but will replace it. I received it back last week on Wednesday and say the repair info and they wrote that gas flow is fine and worked properly and that they fixed spark gap and tightened the loose electrical connections. The fact that the main reason I sent it in was because gas flow issues and nothing was addressed had me worried. I tested it this past Saturday and the gas flow worked great for about 5-10 seconds and then it stopped again just like it had before. I then tried calling alex and lest a message and emailed as well but haven't heard anything yet but of course it's the weekend so I wasn't expecting immediate reply.
Anyway, have any of you experienced this and know of a remedy? I'm going to try and contact alex again but I'm not looking forward to having to send it back in and wait 2 weeks. I have projects piling up and time is running out. It seems that the solenoid is jamming however I think it is not due to debris but an actual mechanical issue with the solenoid. The green led inside the machine for the solenoid turns on and off when power is applied so that tells me it's seeing power and the solenoid is opening and closing but it seems it's only opening a fraction and jamming as verified by the tests we did.
So again, any suggestions? Hopefully I'll get to speak with Alex later today.
Also, so it's known, I'm not bashing everlas or anyone affiliated, the service I have received has been pretty good I'm just frustrated because I spent a good amount of money on something and it's been a month now and haven't gotten to enjoy it.![]()
Thanks guys and sorry if there are grammatical errors, typed this from my phone. Heh




Reply With Quote