Quote Originally Posted by performance View Post
Sait, is ok, but I found that Pearl abrasives makes a fantastic disk for grinding. That's what I use. They are fast grind, long life wheels, and have a funny red color to the unit. They also have a special SS grinding wheel that improves performance on SS.
Well, I googled them and found them at EMI supply for $1.65 each. So I ordered 50 to try.

EMI is giving away free samples of ARC abrasives, so I ordered those as well.