Share
Results 1 to 2 of 2

Thread: Scuba Tank Cart

  1. #1
    Join Date
    Feb 2011
    Location
    West Palm Beach Fl.
    Posts
    68

    Default Scuba Tank Cart

    Click image for larger version. 

Name:	DSC02091.jpg 
Views:	913 
Size:	147.8 KB 
ID:	1300Click image for larger version. 

Name:	DSC02092.jpg 
Views:	828 
Size:	148.8 KB 
ID:	1301 I made this tank cart last year for lobster mini season. I can put 8 tanks in it and roll it almost anywhere. The frame work that holds the tanks is 1/2" conduit bent and brassed together, the deck is 1/8" aluminum diamond plate welded to 1 1/8" x 1/8" aluminum angle. The main frame 1"x 1 1/2" steel square tubing. The wheels are from HF and are mounted on 5/8" steel rod. Having the wheels under the deck allows them to turn sharply. This makes for easy manuvering on the dock or in the parking lot.If you have ever luged a dozen tanks back and forth, at the end of July in Florida, you know how handy this thing can be.
    Power Tig 250 EX
    Miller 211 Mig
    Hobart Stickmate LX
    Victor Torch

  2. #2

    Default

    I hate lugging my gear and single tank around, this would be an awesome tool. I would probably use wider tires on mine since Michigan doesn't always have smooth and level approaches to the water (shore diving) and sand would be quite tricky with the weight of a couple tanks on the narrow tires.

    Great work BTW!!
    Build it, wheel it, break it, fix it, and repeat!!!!!!!

    Tools:
    Everlast SuperCut 50 Plasma
    Century 200 Mig welder
    JD2 Model 32 Tube Bender

    Toys:
    1995 Ranger 2wd regular cab - 5.0HO Conversion - Street Machine
    1993 Ranger SuperCab - 466 BBF - Extreme offroad
    1985 F250 Regular Cab 4x4 - 460 BBF - Towing Beast

Similar Threads

  1. How much gas is in the tank?
    By jpmitch in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 11-28-2013, 02:02 AM
  2. Welding Tank Cart
    By Kempy in forum Other Custom Fabrications
    Replies: 13
    Last Post: 02-10-2013, 01:23 AM
  3. Welding Cart - Power Cart 250 - opinions?
    By ScottRussell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 12-05-2012, 01:19 PM
  4. Replies: 15
    Last Post: 08-02-2012, 01:30 PM
  5. Get the biggest tank you can....you won't be sorry.
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 41
    Last Post: 10-13-2011, 07:52 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •