I would say it was caused by lack of fusion at the root of the weld and cracked from the inside out from it flexing
I would say it was caused by lack of fusion at the root of the weld and cracked from the inside out from it flexing
Lincoln precision tig 275
Miller Syncrowave 350 Tig
Miller 250 Mig
old miller 200 Mig
HF 151 Mig
HF 100 FC
Victor Journeyman Oxy/Ace set up
Bunch of tools of the trade to much to list