Well,
I received my PowerTIG 225LX today! The good news it came one day early. Cool! Bad news is, there was some shipping damage. The exterior box was in reasonably good shape so I accepted it from UPS. When I popped the shipping box open. The accessory box contained within was burst and the cable foot pedal, torch spares were everywhere. The welder itself had a cracked rear plastic cover/fan shroud and one of the case screws had popped out and was missing. I placed a call and sent an email to Everlast but haven't heard back from them, probably due to the holiday. I guess now is as good a time as any to see how good their customer sevice is while I still have return priviledges
. I'll keep everyone advised...
Zoom




. The exterior box was in reasonably good shape so I accepted it from UPS. When I popped the shipping box open. The accessory box contained within was burst and the cable foot pedal, torch spares were everywhere. The welder itself had a cracked rear plastic cover/fan shroud and one of the case screws had popped out and was missing. I placed a call and sent an email to Everlast but haven't heard back from them, probably due to the holiday. I guess now is as good a time as any to see how good their customer sevice is while I still have return priviledges
. I'll keep everyone advised...
Reply With Quote