  1. #1

    Default I want a CNC welder

    I want one of these things so bad. Cant afford one. No room to put one. But I got a ton of things I would build with one. Maybe some day. Forget building a dream house. I can live in a garage.
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  2. #2

    Default

    You could always build yourself one. I am in the works of building myself a CNC Mill so I can start making parts. So far I have the total cost to be around $600-$800. Much cheaper than buying one.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  3. #3

    Default

    Hello Jason,

    I have seen a couple conversions. Ide be interested in seeing what you got. Ide love to learn all about converting a machine. I have a minimachine. It works for what I need. However, a CNC can do all sorts of curves so easily. I got to start making money off of one of my inventions before I can justify a CNC. But if I ever get anything going it will be one of the first things I get.
    Last edited by Nikola Tesla; 04-04-2011 at 09:48 AM. Reason: spelling
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  4. #4

    Default

    Well I have not really converted anything into a CNC. I purchased 5 Nema 32 stepper motors and a board that is a controller/5 driver all in one from ebay. Also got a power supply from there. I got it all for around $550 after shipping. The software is normal CNC software. I have been playing with Inventor, solidworks, mastercam and will probably use mach3 for running the machine unless the controller will run off mastercam. Having 5 motors and a controller/driver for that, I will build me a 5 axis mill. The same setup can be used for a lathe or other things if you wanted.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  5. Default

    i'd be very interested in seeing how the mill part of that works out.
    everlast i-mig 200
    96 gmc extended cab truck 350 rwhp daily driven for 289,000 miles
    88 jeep cherokee custom built by me for me for well everything.someday it'll be finished
    4.6L stroker,dana 44 front, 14 bolt rear, 35"xterrains,soon to come 231/205 doubler

  6. #6

    Default

    maybe later I can get some pics of how I have mine setup but all I have at this time is the electronics and there is more than 1 way they are done. I have played around with all the software and have had success with making some parts in them. I should design the table setup in a cad program and see what I come up with. I got an idea in my head of what I want to do so we will have to see. If anyone wants to ask questions I can answer what I know but it may not be much.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  7. #7

    Default

    I was wondering if anyone knows do the submurged arc machines use a sheilding gas under the water or just the water itself to sheild the weld?
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  8. #8

    Default

    Quote Originally Posted by Cippee View Post
    I was wondering if anyone knows do the submurged arc machines use a sheilding gas under the water or just the water itself to sheild the weld?
    Sub arc has nothing to do with water. The arc is submerged under powdered flux while welding. The filler is hot wire or hot strip (hot meaning it is carrying the welding current that is causing the heat to melt the filler). Wire is like a mig process (although usually a fairly large diameter wire). Strip is usually a .020" X 1" wide (or similar size) strip of filler metal and is typically used for weld cladding. The flux selection is important in that it can contain a variety of alloying elements as well as shielding the weld itself (similar to stick welding).
    Last edited by sportbike; 02-19-2012 at 12:56 AM.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  9. #9

    Default

    Wow that is very interesting. What is it called when they weld in like 6" of water? I've seem it on tv before when they weld huge slabs of steel.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  10. #10

    Default

    I want a cnc there not to bad can do one for under a 1000 . they have some good deals on ebay with the controller box and actuators. got a nice on like 4x4 for under a 1000 ready to use just have to have software and plasma cutter .

  11. #11

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I want a cnc there not to bad can do one for under a 1000 . they have some good deals on ebay with the controller box and actuators. got a nice on like 4x4 for under a 1000 ready to use just have to have software and plasma cutter .
    Do you have a link to the P4x4 $1000 CNC, guess I can go dig in tools. What size is it, 2x2.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  12. #12

    Default

    I am getting my table from these guys , they have actions some time seen the kits go as low at 800 bucks normal price with everything exep plasma cutter like 1500 . http://www.ebay.com/itm/CNC-Plasma-C...item2ebcfb6700 there score is not 100 pecent only because people buy these kits and dont know how to put together or dont know how to work cad lol then bitch, thank god i have a friend that's teaching me how to use cad oh this is 4X4 TABLE KIT
    Last edited by Rodsmachineshop; 04-05-2012 at 05:54 PM.

  13. #13

    Default

    I have a friend that built his I was trying to buy. But mailed him for his input. Nice to have friends like that.

    That is the same place that had the 2000 unit complete.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Mystery Welder Revealed: 2012 DIGITAL POWERTIG 210EXT TIG/STICK welder
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 46
    Last Post: 07-28-2012, 03:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •