Share
Results 1 to 15 of 15

Thread: SATAN z31... My car

  1. Default SATAN z31... My car

    I figured I would post this since I just purchased an Everlast 225LX and plan on being here a bit.

    This is my car. I have been working on it for many years. Now copy and paste time....

    Car is a 1985 300zx turbo A.K.A. SATAN Z31

    I ran the car to an 11.55 @ 121.x back in 2005. I recently just ran again in 2010 and pulled a 10.3 @ 134mph.
    http://www.youtube.com/watch?v=leUB4PCv0mU

    I do all of my own fabrication on parts, header's/manifolds, intake, IC piping, exhaust etc.

    Mods performed. (Stuff changes all the time)


    ENGINE
    Block
    Block bored to accept JE 87.5mm pistons
    Block oringed for head gasket reinforcment
    Copper head gaskets
    ARP main girdle studs
    ARP head studs
    Polished crank journals
    Crank slightly lightened durring balancing process
    Eagle rods
    JE forged pistons
    Rotating assembly balanced
    Shimmed oil pump spring for higher pressure

    Heads and Intake
    Exhaust (heads) ported and polished to 38mm with flat valve guides
    Intake (heads) ported and polished to 38mm with flat valve guides
    Ferrea 1mm over sized stainless valves
    Combustion chamber polished-ish
    Exhaust manifolds ported 1mm larger than heads
    Isky race cams over .5" lift over 280* duration
    schneider dual valve springs
    Titanium retainers
    Hydraulic lifters shimmed into solid lifters.
    Russ gears with cams dialed in by dial indicator
    4 angle valve job
    Intake manifold port matched to heads
    Custom plenum to 6 liters.
    Q45 throttle body
    All gaskets port matched

    Rest of Engine
    Custom SATAN tubular stainless manifolds
    Borg Warner S374 turbo 74.5mm turbo
    HKS knock off 50mm waste gate
    4" Turbo back exhaust with muffler
    3" IC pipes from turbo to TB
    12"x24"x4" bar and plate IC with 3" in and outs
    Tial knock of 50mm BOV
    26 1/8"x 20"x3" aluminum radiator
    Custom water catch can
    oil catch can off of valve covers
    Ford Taurus E-fan
    Engine lowered 1.5" with solid mounts
    1/4" steel scatter shield


    Engine management and fuel system
    AEM stand alone for z32 custom wired for z31
    Sazuki Hayabusa ignition coils for coil on plug.
    Z32 cam sensor mounted in z31 distributor
    HKS DLI capacitive discharge ignition box.
    AEM peak and hold driver
    1600cc injectors
    NOS Sniper wet kit
    Walbro 255 feeding surge tank.
    Magnafuel 4303 pulling from surge tank feeding injectors
    1/2" red anodized aluminum fuel line
    Racing fuel filter with replaceable element
    -8 stainless braided hoses with all AN fittings
    Custom 1/2 I.D. fuel rails by me
    Magnafuel fuel pressure regulator
    1/2" red anodized aluminum return line
    Denso 22 and 24 heat range plugs


    Additional Electronics
    AEM Boost control solenoid
    AEM wide band O2 sensor
    Flip button two step integrated with AEM
    Flip switch for high/low boost
    Flip switch for fuel pumps on/off
    Flip switch for datta log on/off
    Flip switch for N2O
    Covered race switch for line lock
    Autometer boost gauge
    APC oil pressure gauge (block tapped to accept 1/8" NPT)
    Auto meter tachometer with shift light
    Battery on/off switch at rear of car
    Sony viao lap top to tune AEM EMS
    Optima Battery relocated to rear driver side of car

    Suspension, chassis and brakes
    Z3R type 2 springs
    Tokico illumina shocks 5 way adjust
    Poly sway bar bushings
    poly sway bar end links
    Poly tension rod bushings
    Poly spring seats
    Drag bags in springs
    10 point roll cage welded in, also additionally welded to A-pillars and to roof.
    90 TT calipers
    350z Track rotors
    brackets for 240sx to move out TT calipers for 350z 12.75" track rotors
    Axxis ultimate brake pads
    Stainless braided brake lines

    Cosmetic/interior/exterior
    Fake nismo race seats
    SFI 5pt harness for driver
    SFI fire suit
    SFI helmet
    SFI fire gloves
    SFI window net
    four point harnesses for passenger
    Quick release steering wheel
    Aftermarket ebay special steering wheel
    Digi dash now cobalt blue
    Cage painted black
    Hole cut in front bumper
    Access hole cut for fuel pumps
    Dash hacked for roll cage
    T-tops rigged to work with roll cage
    hatch glass painted black

    Drive line and clutch
    Clutch specialties 900ft/lb clutch
    Custom aluminum flywheel
    Cr-Mo drive shaft
    Mark Williams 4140 Cr-Mo through hardened axle stubs
    R30A tranny (88 turbo)
    LSD from 88T converted to 6 disk clutch
    Reinforced axle's with 4130 tubing
    Whole rear subframe from 88T
    1/4" steel drive shaft safety loop
    Cobra R wheels 17x9 rear 17x8 front
    Nitto 555 255/40/17 rear
    Nitto 455 235/40/17 front
    M/T ET Drags for track
    M/T ET Streets for street events at track


    Things removed from car
    Damn near everything not needed to run the car
    Complete AC system
    complete Heater system
    Power steering
    Rear interior
    headliner
    complete stereo
    horns
    heat shields
    some sound deadening stuff
    bunch of other stuff too.

    cage welded to roof

    cage welded to a-pillar

    Engine,






    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  2. Default








    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  3. Default

    4" with room to spare!


    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  4. Default

    I just repainted the car my self using HVLP guns and Satin black Urethane paint. I have about 60 hours just in body work alone, and my car wasn't even THAT BAD. I now have a new found respect for any body guy who is worth a ####.

    BEFORE


    AFTER

    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  5. Default

    Our cars are as far from each other as possible and still be cars. Mine runs close to the same times, but has no headlights no turn signals no brake lights, no wiring other than enough to make it start, no guages, no speedo, I wanted it to be least possible car that still functioned. No windshield, no side glass, no top, no bumpers. No paint, and I wash it with windex and a shop towel.
    My wife recently made me put an alternator on it, and I did hook up the front brakes just to shut everyone up. So I now have two luxury items, front brakes and an alternator. There are a few things like 5point harness and the quick release wheel we have in common.

    Yours is a beautiful car.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  6. #6

    Default

    Awesome project man!
    Loving that custom manifold work, art, I say!
    300whp FWD 94 Celica
    PowerPro 205 with a hack behind the mask!

  7. #7

    Default

    Nice work
    Did you fab the manifold and tank(s) yourself?
    Last edited by Ram48; 03-19-2011 at 03:48 PM. Reason: typo

  8. Default

    Quote Originally Posted by Ram48 View Post
    Nice work
    Did you fab the manifold and tank(s) yourself?
    Any welding that has been done on this car (after it left the factory) has been by me.

    Aluminum sheet metal intake
    Stainless tubular headers
    Intercooler piping
    exhaust piping.
    Roll cage
    Fuel surge tank
    4130 sleeved Chromoly axles.
    Misc. stuff here and there.

    I also make all of these parts for customers who own z31's as well. That is how I pay for my race car. The z31 300zx has a very large cult following but not very many aftermarket parts available. So I make stuff people want.
    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  9. Default

    NICE!
    Another Nissan guy on here! (along with Eugene! lol)

    I have a 96 S14 myself... Have an LS1 sitting in another S14 waiting for a transmission.
    But that comes after my cherokee project now.

  10. #10

    Default

    Quote Originally Posted by DiabolicZ View Post
    Any welding that has been done on this car (after it left the factory) has been by me.

    Aluminum sheet metal intake
    Stainless tubular headers
    Intercooler piping
    exhaust piping.
    Roll cage
    Fuel surge tank
    4130 sleeved Chromoly axles.
    Misc. stuff here and there.

    I also make all of these parts for customers who own z31's as well. That is how I pay for my race car. The z31 300zx has a very large cult following but not very many aftermarket parts available. So I make stuff people want.

    I know that feeling all to well. My son and I run an SRT-4 neon drag car that turns 10.3 at 143 and parts were hard to get when they (Dodge) were still building them, now it is almost impossible and some things are just not made so I have made many parts for our car. I have paid for my bead roller and Box and pan brake by doing some aluminum interior skins for other SRT guys. Its nice to be able to support, even partially, your hobby doing what you enjoy

  11. #11

    Default

    sheetmetal fab? I'm in! what kind of box/pan brake you got? and bead roller? I have been looking for a starter set, I wanna build some inner fenders and interior skins for my bronco project. never done sheet metal before, could use some helpful info.
    I'd like to think I'm the guy they are talkin about when they say, "he could F%^& up a cannon ball in a plowed field."
    .................. /...\
    ..............-...|.....|
    ...*.......-'. \..\__/
    ....\.-'.........\
    ... /......... _/
    ...|......... /"
    ...|.... /_\'
    ....\....\_/
    ......""""

  12. #12

    Default

    Nice work, and a nice toy...

    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  13. #13

    Default

    Quote Originally Posted by ScratchStart View Post
    sheetmetal fab? I'm in! what kind of box/pan brake you got? and bead roller? I have been looking for a starter set, I wanna build some inner fenders and interior skins for my bronco project. never done sheet metal before, could use some helpful info.
    Box and pan brake is from Enco. and the bead roller was made by a felow named Tom, he is known as courtjester on youtube he just finished another style and may want to sell the last one he built. Look him up or if you want give me your contact info and I will pass it on.

  14. #14

    Default

    Sweet car, fab work is top notch. Gotta love the sound a turbo drag car makes down the track!!!!!

    From the video it does look like a little fine tuning on the rear suspension good get you to the big end a little quicker. A couple hops caused excessive wheel spin at launch. Badass for sure though.
    Build it, wheel it, break it, fix it, and repeat!!!!!!!

    Tools:
    Everlast SuperCut 50 Plasma
    Century 200 Mig welder
    JD2 Model 32 Tube Bender

    Toys:
    1995 Ranger 2wd regular cab - 5.0HO Conversion - Street Machine
    1993 Ranger SuperCab - 466 BBF - Extreme offroad
    1985 F250 Regular Cab 4x4 - 460 BBF - Towing Beast

  15. #15

    Default

    Box and pan brake is from Enco. and the bead roller was made by a felow named Tom, he is known as courtjester on youtube he just finished another style and may want to sell the last one he built. Look him up or if you want give me your contact info and I will pass it on.
    I found him on youtube, that guy is awesome! sent him an email, waiting for his reply.

    thanks for the info, between this guy and Jody(weldingtipsandtricks.com), I'm already a pro...LOL
    I'd like to think I'm the guy they are talkin about when they say, "he could F%^& up a cannon ball in a plowed field."
    .................. /...\
    ..............-...|.....|
    ...*.......-'. \..\__/
    ....\.-'.........\
    ... /......... _/
    ...|......... /"
    ...|.... /_\'
    ....\....\_/
    ......""""

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •