Share
Results 1 to 20 of 35

Thread: Press brake

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Press brake

    It is the SWAG off road kit. I have to modify it for my press by extending the tabs you see on the front and re welding the clamping ears. (it seems to work fine without them so we will see if I need to do that) the HF 20 ton has 4 inch side beams and my Arcan has 7 inch wide rails and is rated for 30 ton even though it had a 20 ton jack, I added the 20 ton Air over Hydraulic you see in the picture.
    Please give me feedback on the welds as I'm still learning
    I mig 200
    1/4 mild steel
    175 amps
    22 volts
    0.35 solid wire
    75 / 25 mix
    The test bends were on 3/16 mild steel and there was no resistance at all. I like this tool.
    Ray
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	press brake 007.jpg 
Views:	602 
Size:	115.2 KB 
ID:	1051   Click image for larger version. 

Name:	press brake 005.jpg 
Views:	625 
Size:	91.6 KB 
ID:	1052   Click image for larger version. 

Name:	press brake 004.jpg 
Views:	598 
Size:	91.0 KB 
ID:	1053   Click image for larger version. 

Name:	press brake 001.jpg 
Views:	697 
Size:	82.9 KB 
ID:	1054   Click image for larger version. 

Name:	press brake 003.jpg 
Views:	616 
Size:	82.5 KB 
ID:	1055  

    Click image for larger version. 

Name:	press brake 002.jpg 
Views:	620 
Size:	67.3 KB 
ID:	1056  
    Last edited by Ram48; 03-08-2011 at 06:35 PM. Reason: added welding information

Similar Threads

  1. Brake project
    By chadford in forum Other Custom Fabrications
    Replies: 13
    Last Post: 07-22-2011, 03:45 PM
  2. Press for the brake. $35 total, that was for the jack.
    By chadford in forum Other Custom Fabrications
    Replies: 10
    Last Post: 07-19-2011, 11:17 AM
  3. Press brake for modified HF shop press
    By Scooter in forum Other Custom Fabrications
    Replies: 18
    Last Post: 06-06-2011, 07:29 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •