    Default Electric Wall Heater Repair

    I did a quick welding repair job today on an old electric wall heater that had a damaged heat exchanger, which was obsolete (no longer available.) The ~50 year old heat exchanger became bent (not shown) due to excessive heating (from previously replaced components in the heater, such as the fan motor) and customer had cold straightened, leaving some cracks in the aluminum alloy I quickly and partially TIG welded (crack repair not shown.)

    Curiously, the heat exchanger mounting brackets were also about 1/4" too tight, so I repositioned one of them by cutting it off from the rest of the sheetmetal frame (4.5" angle grinder w/ cut-off wheel) and re-welded the bracket back on to the frame in a new position. Resulting in the heat exchanger able to be installed without stress.

    As the bracket / frame was pretty thin sheet steel (I didn't measure but would guess perhaps .050" or so), I used some aggressive pulse settings (minimum pulse background current, and minimum pulse duty cycle, and minimum pulse frequency) to minimize heat input and oxidation, while welding it up in one quick pass. I used 1/16" 309L stainless filler rod, a #6 gas lens with ~13 cfh argon, and a really sharp 1/16" tungsten electrode.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0003_small.JPG 
Views:	571 
Size:	94.4 KB 
ID:	1026   Click image for larger version. 

Name:	IMG_0001_small.JPG 
Views:	546 
Size:	40.9 KB 
ID:	1025   Click image for larger version. 

Name:	IMG_0002_small.JPG 
Views:	526 
Size:	53.9 KB 
ID:	1027   Click image for larger version. 

Name:	IMG_0004_small.JPG 
Views:	584 
Size:	84.3 KB 
ID:	1028  
    Last edited by jakeru; 03-06-2011 at 10:23 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. Solar Water Heater
    By ShaneJackson in forum Personal Projects (no welder required)
    Replies: 46
    Last Post: 02-22-2013, 07:58 AM
  2. Wall art , first real tig project.
    By Ram48 in forum Metal Art
    Replies: 15
    Last Post: 05-13-2012, 01:41 PM
  3. New Water Heater
    By Powertig in forum Personal Projects (no welder required)
    Replies: 11
    Last Post: 05-03-2012, 03:57 AM
  4. Replies: 5
    Last Post: 01-04-2012, 02:03 AM
  5. Electric Scooter fork repair
    By chadford in forum Welding Repairs
    Replies: 0
    Last Post: 07-08-2011, 05:51 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •