Originally Posted by
everlastsupport
I use a 250P for most of my MIG welding and I never use the pulse controls. Never had a reason and never been disappointed in a weld it's done. I wish the 250P went lower than 40amps as that's a tad to hot for sheet metal.
The 205P would be a good choice for those doing sheet metal to 1/4"-3/8" steel (single pass) but still want the pulse mode. Not a bad range.
If you have the extra cash, nothing wrong with the 205P. But I agree with Mark, I too would probably skip the pulse unless I could not get the unit I wanted without it.