    Found another old automotive welding project I wanted to share.

    I had a rear anti-swaybar bracket on a car frame break, apparently from the original bracket not being strong enough for the stiffer aftermarket anti-swaybar. It broke on the edge where the bolt went through the bracket. The bracket material was simply not thick and strong enough.

    So I not only weld repaired the crack, but I added a reinforcing piece of angle iron, that was approx 1/8" thick. I TIG welded it into place, and did the same on other bracket on other side. The reinforcement substantially increased the rigidity of the bracket, as applying force on the bracket by hand, it would not flex noticeably at all with the reinforcement added. As pictured, it still needed some paint to protect from corrosion.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0007.jpg 
Views:	491 
Size:	138.4 KB 
ID:	1018  
    '13 Everlast 255EXT
    '07 Everlast Super200P

  2. Default

    That looks like you have some sort of lift kit installed. What vehicle is it on? Good idea in the reinforcement by the way.
    Miller Dialarc 250
    ESAB Migmaster250
    Smith Heavy Duty OXY/ACETYLENE outfit
    Arcair gouging set

Similar Threads

  1. Anti-roll bar link mounts
    By its_34 in forum On Road Fabrication
    Replies: 5
    Last Post: 08-17-2013, 04:42 AM
  2. Cast Aluminum Repair on Lathe Bracket W/ Power Tig Micro 185
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 10-20-2012, 05:15 PM
  3. RV Mudflap Bracket - TIG welding
    By jakeru in forum On Road Fabrication
    Replies: 4
    Last Post: 04-17-2012, 05:26 AM
  4. Replies: 2
    Last Post: 08-03-2011, 03:50 PM
  5. Replies: 5
    Last Post: 06-18-2011, 08:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •