    Default Oxy-Acetylene Cutting 1/2" Thick Steel Fire Barrel

    Here is a friend's steel fire containing barrel I oxy-acetylene cut for him, out in his backyard. This was very substantial material; a 1/2" thick galvanized (zinc-plated) steel. He said it was a scrap he obtained that was originally made for some sort of pier footing or support (?) in Alaska.

    He's going to take the cut off ring out to another location, an island vacation cabin where he'll use it for beach fires.

    It would have been fun to use my Super200P's plasma cutter to do this, but the prospect of getting 240V power *and* compressed air out there was just too much. The portability of "old school" oxy-acetylene rig beat out new fancy plasma cutting technology in this case.

    The "smokey" residue around the cut is from the galvanized (zinc layer) burning, and wiped right off, and the brittle slag "dribbles" on the inside of the cut edge also knocked off easily.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0043.jpg 
Views:	482 
Size:	139.7 KB 
ID:	1005   Click image for larger version. 

Name:	IMG_0042_small.JPG 
Views:	407 
Size:	124.2 KB 
ID:	1004   Click image for larger version. 

Name:	IMG_0037.jpg 
Views:	462 
Size:	149.7 KB 
ID:	1003   Click image for larger version. 

Name:	IMG_0041.jpg 
Views:	453 
Size:	151.8 KB 
ID:	1002  
    Last edited by jakeru; 03-04-2011 at 10:24 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. Cutting a 4" circle....
    By CGCINC in forum Everlast Plasma Cutters (PAC)
    Replies: 9
    Last Post: 07-18-2012, 07:18 PM
  2. Anybody cutting 1"?
    By Jake98 in forum Everlast Plasma Cutters (PAC)
    Replies: 19
    Last Post: 05-11-2012, 05:19 PM
  3. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM
  4. "Battlebot" Repair (TIG weld 4130 Cr-Mo steel)
    By jakeru in forum Welding Repairs
    Replies: 4
    Last Post: 03-07-2011, 09:51 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •