    I just wanted to check with some PA 200 users. Did anyone change or add to the length of their holder and ground leads? I asked the guy's at Everlast if 50' would be ok to use and they told me yes which sounds ok to me. I just wanted to see what you guy's are using.
    Thanks

  2. #2

    Default

    I replied to this over on WW. You could go to 100' with #2 cable.
    Everlast PowerArc 300
    Everlast PowerArc 200
    Everlast PowerPlasma 70
    Hobart Handler 125 EZ
    Lincoln Tombstone AC
    Lincoln Tombstone AC/DC
    O/A outfit
    Honda 11K generator

  3. #3

    Default

    Thanks GWD, I checked WW early this morning but did not have any replies so I thought I would do better here. I have some new Carol Super Vu-Tron in #4 I was planning on using. I was going to make them 50'.
    Thanks

  4. #4

    Default

    It turns out that #4 cable is rated to go to 150A up to 100'. The smallest cable size for a 200A application is #2.

    There is probably a "fudge factor" involved but if you don't plan on using more than 150A very often it should be fine.

    Another option is to use the #4 as a 10' to 15' stinger if weight is a factor.

    http://store.weldingdepot.com/pdf/weldingcable.pdf
    Everlast PowerArc 300
    Everlast PowerArc 200
    Everlast PowerPlasma 70
    Hobart Handler 125 EZ
    Lincoln Tombstone AC
    Lincoln Tombstone AC/DC
    O/A outfit
    Honda 11K generator

  5. Default

    Here's a chart.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Welding Cable Chart.JPG 
Views:	883 
Size:	114.4 KB 
ID:	963  

  6. #6

    Default

    That surprises me that #4 is only good for 150 amps, I think I will shorten the ground some to decrease the total length. Most of my stick welding will be 1/8" 7018. I do plan on keeping the cables that come with the machine (they must be #2 ?) for the rare occasion when I might use the ArcAir with some very small carbon.
    Thanks guys

Similar Threads

  1. Welding 1/8 to 3/16 mild steel with powerarc 140st on 120v ?
    By ridenlow559 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-15-2015, 01:58 AM
  2. 12.5' or 25' TIG cable???
    By johnnymg in forum General Welding Questions
    Replies: 13
    Last Post: 08-09-2013, 01:25 AM
  3. welding cable size.
    By bobwills in forum Stick Welding (SMAW)
    Replies: 11
    Last Post: 09-25-2011, 03:05 PM
  4. welding cable gauge
    By Haywire in forum Stick Welding (SMAW)
    Replies: 2
    Last Post: 04-22-2011, 11:45 PM
  5. Automotive Transverse V6 Equal Length Downpipe
    By jakeru in forum On Road Fabrication
    Replies: 3
    Last Post: 03-07-2011, 05:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •