    I made a weld positioner for doing circular tig welds. By mounting a pivoting arm on the base, I find that it works really well for cutting circles with the plasma cutter. Cost of the postioner was zero, all from junk under the bench. Power for the positioner is a small variable speed Makita cordless drill.

    Here I have cut a couple of 18" discs (both at once with the little Power Ultra 205 multi)for a custom drum I have to build. The drum will go into a new machine being built for a large bakery somewhere in Salt Lake City.

    Here is a link to a video clip of the cut http://www.youtube.com/watch?v=iI0qbNjLCHs

    Looks like 28 amps is the setting showing there, not bad for cutting 2 at once (3/16" ea.) which is much tougher than a single thickness of 3/8".

    Glen
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	plasma 2 001.jpg 
Views:	2771 
Size:	94.1 KB 
ID:	931   Click image for larger version. 

Name:	plasma 2 003.jpg 
Views:	1572 
Size:	82.9 KB 
ID:	932  
    Last edited by worntorn; 03-03-2011 at 08:28 PM.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

Similar Threads

  1. Circle Cutter for iPT-60 Torch?
    By ebrandt in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 09-05-2018, 11:24 PM
  2. Plasma Circle Cutter
    By In Utopia in forum Buy, Sale or Trade
    Replies: 3
    Last Post: 01-24-2013, 05:25 PM
  3. Need to plasma cut some circles/holes soon. Cheap magnetic circle plasma jig.
    By everlastsupport in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 05-15-2012, 04:06 AM
  4. Circle cutter recommendations
    By GreenGrass in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 10-26-2011, 03:53 PM
  5. Home made rotisserie
    By Jason in forum Other Custom Fabrications
    Replies: 11
    Last Post: 03-21-2011, 02:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •