    Default home-made weld positioner or plasma circle cutter

    I made a weld positioner for doing circular tig welds. By mounting a pivoting arm on the base, I find that it works really well for cutting circles with the plasma cutter. Cost of the postioner was zero, all from junk under the bench. Power for the positioner is a small variable speed Makita cordless drill.

    Here I have cut a couple of 18" discs (both at once with the little Power Ultra 205 multi)for a custom drum I have to build. The drum will go into a new machine being built for a large bakery somewhere in Salt Lake City.

    Here is a link to a video clip of the cut http://www.youtube.com/watch?v=iI0qbNjLCHs

    Looks like 28 amps is the setting showing there, not bad for cutting 2 at once (3/16" ea.) which is much tougher than a single thickness of 3/8".

    Glen
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	plasma 2 001.jpg 
Views:	2814 
Size:	94.1 KB 
ID:	931   Click image for larger version. 

Name:	plasma 2 003.jpg 
Views:	1607 
Size:	82.9 KB 
ID:	932  
    Last edited by worntorn; 03-03-2011 at 07:28 PM.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  2. #2

    Default

    Very good, I like it , you remind me of me.

  3. #3

    Default

    Any more pictures of the components, that works sweet and I am interested in building one for myself. Thanks
    Build it, wheel it, break it, fix it, and repeat!!!!!!!

    Tools:
    Everlast SuperCut 50 Plasma
    Century 200 Mig welder
    JD2 Model 32 Tube Bender

    Toys:
    1995 Ranger 2wd regular cab - 5.0HO Conversion - Street Machine
    1993 Ranger SuperCab - 466 BBF - Extreme offroad
    1985 F250 Regular Cab 4x4 - 460 BBF - Towing Beast

  4. Default

    I captured the pics so I could reference them later, what we need is a picture of the gearing you used.

    I think I'm seeing a power window track there for the gear down. if that's not what you used, a power window mechanism/motor and a rubber drive wheel should work just fine.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  5. #5

    Default

    I'll take some pictures of the unit tomorrow and post them. I used an old gear reducer and a small part of the remains of a burned out electric garage door opener.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  6. #6

    Default

    Here is a link to another video clip that shows the postioner a bit better. http://www.youtube.com/watch?v=av-aIMH-iFQ

    The flat vertically mounted silver plate is the bottom out of an old garage door opener. I used it for the spindle since the other end of the spindle already had a sprocket of the correct pitch on it. The nylon gear is just along for the ride.
    The cordless drill just gets chucked onto the spindle and then activated by pushing the handle down so that it engages the bolt(ground the head roundish) you see me turn a little bit to change speed. Turning the bolt in and out varies the speed by pushing/releasing the trigger. The gear reducer is a right angle 40 to one unit. The sprockets give another 4 to one, so 160 to one is the total reduction after the drill.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  7. #7

    Default

    How do you attach the ground?
    .
    Eide
    PowerTig 225 LX

  8. #8

    Default

    I just clamp to the table and let it go around with the object being cut or welded. Sometimes I have to stop at about 3/4 the way around and reposition the clamp, not a big deal for the way I use the rig.
    Expensive weld positioners use weld brushes on the pivot shaft for the ground, probably a good idea if you are using a weld positioner day in and day out.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  9. #9

    Default

    Thats a pretty swwet bit of back yard engineering. My kinda thought process. Hope you dont mind some of us Borrowing your idea!
    When opportunity knocks, most do not recognize it, because it shows up wearing overalls and looking like work!!
    Joshua,Tacoma,Wa
    24'x48'shop-6/2010
    Hobart Handler125w/125cf 75/25-1998-Welds perfect
    Power tig250EX-w/300cf argon-2/2011-had 4053 problem, fxed and good as new
    Power Cool W300-4/2011-works great after making hoses
    Power Plasma 50-4/2011-in for repair
    Shop air

  10. #10

    Default

    not a bit, that's why I put it on here. I think it's great when old clutter under the bench can be made into something useful.

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  11. #11
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    Nice work good to see that people still have that bit of creativity left in them. This is just the reason I keep all the treasures ( junk the wife thinks) that I find.

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  12. #12

    Default

    great work Worntorn, I have a similar set-up that I use with a cutting torch I used a Power wheelchair motor with a gearbox that was set up for 24v and just run it at 12v Off a small power supply. it runs about the same speed yours shows and works great. I took the tire off the wheel then mounted a plate to the wheel as my cutting base with the torch set up I dont have to worry about ground but once I get my plasma cutter I will probably have to make a brush set up like your talking about.
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  13. #13

    Default

    thanks Don

    With the variable speed on the drill the rpm of the plate can be adjusted from almost zero to a max of 15RPM and anything in between.
    The bolt that the speed trigger rests against is the adjuster, it can be threaded in and out easily with index finger and thumb.

    Looks like I may be using it quite a bit, I have another custom feed wheel to build for the Bakery Equipment Supply company.

    Glen
    Last edited by worntorn; 03-23-2011 at 03:17 AM.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  14. #14

    Default

    yea I cant wait for my 250ex to arrive I have a few projects that I will put it to good use on. Yours is definitely more adjustable but I just use mone to cut out the round sides for smoker bbq's was making . got a bunch of freebie food grade steel drums and had to make my own fire boxes for the coals and the smoke wood. They worked out great while I had em. outta drums and the ones that have oil or other chemicals and such cant be used cause you have to heat them so hot to burn out any residue and I don't have that capability. wouldn't want to poison anyone. I got 4 people waiting on me to make them extended drag swing arms, good coin there and I also have a Pucati 999r that I need to tear down and make a frame jig and Ill be making a new frame in Titanium. should drop some weight from the stock steel trestle frame.

    The red parts will all be redone in titanium at some point

    Attachment 1303

    so many projects so little time LOL.
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  15. #15

    Default

    why don't you use one of these and ground the shaft?

    attach it to a bolt on one end and put a spring on the other so it holds tension against the shaft, then just hook your plasma/tig ground to the bolted down end?

    I can't remember where I have seen this, but I have used it a couple times when welding broken shafts back together in a lathe, works great
    I'd like to think I'm the guy they are talkin about when they say, "he could F%^& up a cannon ball in a plowed field."
    .................. /...\
    ..............-...|.....|
    ...*.......-'. \..\__/
    ....\.-'.........\
    ... /......... _/
    ...|......... /"
    ...|.... /_\'
    ....\....\_/
    ......""""

  16. Default

    Brilliant! I have a 90 degree gearbox that I've wanted to set up as a positioner for tubing-type work. I gave up un the project a while back becuasa I didn't have a cheap easy way to drive the thing. It just so happends nthat I have a coulpe of cordless drills with dead batterys laying around. I will be starting a thread on powering them, up with regular AC. Thnaks!!
    Miller Dialarc 250
    ESAB Migmaster250
    Smith Heavy Duty OXY/ACETYLENE outfit
    Arcair gouging set

  17. #17

    Default

    Thats a really good Idea using a variable speed drill connected to a gear box, I think I'm going to borrow that. Thanks
    James Swanson

    Millermatic 135
    (saving for a Power pro 256)
    Linde HDA200
    Custom water cooler and cart

  18. #18

    Default

    no problem.

    I use the little weld positioner all of the time now. It gets used roughly 50/50 for welding and plasma. I built it with welding in mind, but the addition of the pivoting arm made it quite useful for cutting circles or part circles with the plasma cutter.

    Next I added an steady rest for the forearms to lay on when tig welding. This is just a 10" long block of 2x 10 placed on edge and fastened along the side of the metal base plate. The block sits about 1/2" from the turntable at the closest point.

    I just realized that you can see the block in the video, guess it was already on there when I filmed that.

    Anyway, in case anyone wondered, that is what that wooden block is for!

    ScratchStart, good idea, I 'll give that a try.
    Most of the time just clamping the ground to the turntable works fine, but once in awhile I'm doing something where it gets in the way.
    Glen
    Last edited by worntorn; 04-29-2011 at 02:43 AM.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  19. #19

    Default

    I really need to build something like this. It will save me tons of time cutting circles out of 3/8 steel for hubs.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  20. #20

    Default

    It didn't take long to build, started in the morning and was playing with it in the afternoon. I already had all of the necessary bits on hand, that helped.

    If you have any questions on how to build it or what to use, just ask away , be glad to help.

    Glen
    Last edited by worntorn; 06-22-2011 at 02:20 AM.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

Similar Threads

  1. Circle Cutter for iPT-60 Torch?
    By ebrandt in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 09-05-2018, 10:24 PM
  2. Plasma Circle Cutter
    By In Utopia in forum Buy, Sale or Trade
    Replies: 3
    Last Post: 01-24-2013, 04:25 PM
  3. Need to plasma cut some circles/holes soon. Cheap magnetic circle plasma jig.
    By everlastsupport in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 05-15-2012, 03:06 AM
  4. Circle cutter recommendations
    By GreenGrass in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 10-26-2011, 02:53 PM
  5. Home made rotisserie
    By Jason in forum Other Custom Fabrications
    Replies: 11
    Last Post: 03-21-2011, 01:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •