Thread: 4130 BMX bicycle bottom up build

  1. #1

    Default 4130 BMX bicycle bottom up build

    Here is my bmx build. It was a fun build, figuring out the jig was a blast. I look forward to making many more bicycles.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	sick.jpg 
Views:	449 
Size:	78.5 KB 
ID:	621   Click image for larger version. 

Name:	rear triangle in jig.jpg 
Views:	416 
Size:	69.1 KB 
ID:	622   Click image for larger version. 

Name:	chainstay fit up.jpg 
Views:	441 
Size:	57.9 KB 
ID:	623   Click image for larger version. 

Name:	fun gusset.jpg 
Views:	430 
Size:	42.9 KB 
ID:	624   Click image for larger version. 

Name:	freshly welded still in the jig.jpg 
Views:	438 
Size:	61.7 KB 
ID:	625  

    Click image for larger version. 

Name:	fu tube.jpg 
Views:	417 
Size:	74.7 KB 
ID:	626  

  2. #2

    Default

    Nice build, it's easy to see you have talent. I just bought a JD notch master for notching some tubes, what material did you use for your build.

  3. #3

    Default

    Thanks,
    The material is 4130 bought at an avataion supplier, Aircraft Spruce. I have used tube notchers and they work great. I made a v block for my tool post and I cut the tubing on my lathe using my chuck to turn a hole saw at low speed. I can cut huge angles and offsets easily.

Similar Threads

  1. Monday morning quarterback: bicycle weld
    By DaveO in forum General Welder Questions
    Replies: 4
    Last Post: 04-08-2013, 07:04 PM
  2. Filler metal selection for welding mild steel and 4130 tube
    By hooda in forum General Welding Questions
    Replies: 11
    Last Post: 03-21-2013, 07:38 PM
  3. Foot Pedal Bottom Pad
    By NRM in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 17
    Last Post: 08-22-2012, 10:46 PM
  4. Has anyone built a bicycle before, from scratch?
    By CGCINC in forum General Welding Questions
    Replies: 7
    Last Post: 05-08-2012, 01:00 PM
  5. Replies: 7
    Last Post: 10-09-2011, 07:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •