  1. Replies
    5
    Views
    4,949

    Thanks for the input on the cart. I'm going to...

    Thanks for the input on the cart. I'm going to use some leftover tube to make a short rod holder.

    On the pics, they were taken in landscape and rotated when I uploaded them from my iPhone.
    ...
  2. Replies
    5
    Views
    4,949

    Tig Welding Cart

    Started out with a Harbor Freight Welding cart for about $35.00

    Modified it to work with my Powertig 185

    Still have some things to add and a few minor changes.

    118061180711808

    Anyone...
  3. Very cool and unique ideas you have. Thats why I...

    Very cool and unique ideas you have. Thats why I love the web and these type forums so much. A brain trust of some cool and unique ideas!

    Keep up the good work.

    Glenn in GA
  4. Replies
    19
    Views
    16,900

    Very cool, thanks for all your information and...

    Very cool, thanks for all your information and the pictures. I have a table I am building at the house. Will post pics soon. I had the local shop cut a 2'x4' 1/2" thick top with rounded corners...
  5. Replies
    4
    Views
    5,876

    Long time and finally an update! Finally got...

    Long time and finally an update!

    Finally got the 220 ran and powered up the 185. Very smooth and easier to control. This welder came alive on 220. Also max amps are 193 for mine. Smoother...
  6. Replies
    15
    Views
    7,660

    I have seen and heard of them, but never use...

    I have seen and heard of them, but never use them. The 1.5 Lant (Gold Band) is very close to it, just does not have the added rare earths. Never welded with either.

    Glenn
  7. Replies
    15
    Views
    7,660

    Yes it's 2'x4' with 22 1"x6" slots 1/2" thick. ...

    Yes it's 2'x4' with 22 1"x6" slots 1/2" thick. Shop I used has a laser that can handle 1" thick steel. I pick it up on Thursday (have to work tomorrow). I am really excited about it.

    I am in...
  8. Replies
    15
    Views
    7,660

    Ok, update. Visually looking I can't really...

    Ok, update.

    Visually looking I can't really tell much of a difference in the one I spun on the drill VRS the one I hand turned. I did change the grind so that the wheel was spinning towards the...
  9. Replies
    15
    Views
    7,660

    Yep, I put it in two forums hoping for a broader...

    Yep, I put it in two forums hoping for a broader base of experience and answers.

    The wheel he ordered is 180 grit if I remember right. I just ordered an 800 grit diamond 4" to fit my angle...
  10. Replies
    15
    Views
    7,660

    WOW, just saw the title. Sharpending LOL The...

    WOW, just saw the title. Sharpending LOL

    The tank could be contaminated I guess, I got it from my local supplier, its deff labeled as Argon and what welds I have done are clean (steel and...
  11. Replies
    15
    Views
    7,660

    Tungston Brand Quality and Sharpending Methods

    Has anyone done a comparison on tungston quality? I can get very cheap tungston from weldingcity.com in 2% Blue (what I am liking so far). However I am wondering if it's good quality. Do the name...
  12. Thanks for the report. The Everlast Amptrol, it...

    Thanks for the report. The Everlast Amptrol, it gas a power switch, then a separate roller to adjust the amps?

    Glenn
  13. All this pot talk makes me want to cook or smoke!...

    All this pot talk makes me want to cook or smoke!

    So if I'm reading you correctly, the new 185 can use a 25k ohm pot and it should work correctly?

    CK makes a fingertip control for Hobart that...
  14. I would love to have a 3d printer. By the time I...

    I would love to have a 3d printer. By the time I get around to that they will be even better and more affordable.

    Pulled off the cover and just checked out the guts of the foot pedal. By the...
  15. When I say gun trigger, I just mean in how it...

    When I say gun trigger, I just mean in how it actuates. No spring or tension to pull against. Matter of fact, a ring that your finger goes into and can pull and push would be more desirable. That...
  16. I called and spoke with CK's tech support today. ...

    I called and spoke with CK's tech support today. I was told that the current finger remotes will work with the Everlast EXT line, but they could not guarantee it to work with anything else in the...
  17. I have not taken apart my foot controller to...

    I have not taken apart my foot controller to check yet, but from the operation of it, when you first move the pedal a fraction there is a click, which I think it to "turn on the welding power and the...
  18. Which, the Everlast is not 47k or CK is not...

    Which, the Everlast is not 47k or CK is not sourcing a 47k pot?

    Thanks
    Glenn
  19. The new foot pedal has a 47k pot correct? So...

    The new foot pedal has a 47k pot correct?

    So is CK sourcing a new pot to correct the issue?

    Thanks
    Glenn
  20. I have not seen the torch in question, must be...

    I have not seen the torch in question, must be like the one that came with Hobart a few years ago. I was thinking along the lines of the CK one. No on off switch, just a potentiometer (sp) like the...
  21. Replies
    4
    Views
    5,876

    Mark yes I'm in McDonough, did post in one of the...

    Mark yes I'm in McDonough, did post in one of the threads when you said you had come through there a couple of hours ago.

    Having fun with it, just use some copper ground wire and ran some beads...
  22. Check this thread out ...

    Check this thread out

    http://www.everlastgenerators.com/forums/showthread.php/2425-CK-Torch-Packages-For-Everlast-Welders

    Glenn
  23. The fingertip control works just like the pedal...

    The fingertip control works just like the pedal it's just controlled by your finger. The pedal works just fine, so I can't see a reason why the fingertip control would not.

    Thanks
    Glenn
  24. Any news on the fingertip amp control? Glen

    Any news on the fingertip amp control?

    Glen
  25. Replies
    4
    Views
    5,876

    2013 Powertig 185

    Let me see how much I can condense my story so y'all will read this through to the end.

    After a week of phone calls, emails, mobile phone calls and texts between Alex and Oleg (mainly Oleg, even...
Results 1 to 25 of 62
Page 1 of 3 1 2 3