Search:

Type: Posts; User: bobwills

Page 1 of 13 1 2 3 4

Search: Search took 0.01 seconds.

  1. Replies
    5
    Views
    8,147

    Well it's back to making a noise for the first 30...

    Well it's back to making a noise for the first 30 seconds it's on again. It's been inside for a couple hours and welded some So we know it's not still froze.


    Sent from my iPhone using Tapatalk
  2. Replies
    5
    Views
    8,147

    Ive owned a pa 200 for several years and I've...

    Ive owned a pa 200 for several years and I've never seen anything like it. When it turns off the amperage reading dances around reading a bunch of different numbers. The high pitch sound has not...
  3. Replies
    5
    Views
    8,147

    The longer it sits the high pitch noise is going...

    The longer it sits the high pitch noise is going away. The display is still laggy while turning on and flashes numbers for 5 seconds after turning off. I am wondering if it coulda just been froze...
  4. Replies
    5
    Views
    8,147

    New Powerarc 200 st problems

    My buddy just received a new powerarc 200 st and when we turned it on after about 10 seconds a high pitch screeching sound started coming from it. Turned it off and when it turns off the display is...
  5. Replies
    19
    Views
    14,435

    So do drag tips wear quicker since they are...

    So do drag tips wear quicker since they are dragging on the metal when hot or just like the other ones or better.
  6. Replies
    10
    Views
    5,746

    For jobs like that do you charge by the inch or...

    For jobs like that do you charge by the inch or do you now just have a set rate for that person for each mobile home.
  7. Replies
    19
    Views
    9,460

    Thats still a great deal. One you dont run across...

    Thats still a great deal. One you dont run across very often. Do you know how many years old it is?
  8. Funny thing we had to weld some round drain...

    Funny thing we had to weld some round drain covers in that was at a school into its holder because some kid thought it would be funny to pull the cover out and another little kid was walking through...
  9. Project 1 from Bobwills summer rerun. box culvert grates

    I had to make these metal grates for work. There was four of them. Two had to fit in like a 29" hole or something. They were a custom fit. They fin in a wall getting bolted there to keep people and...
  10. Replies
    11
    Views
    6,610

    Very nice. What kind of welding do you do that...

    Very nice. What kind of welding do you do that you need such a hefty welder for. Or did you just want it for all those setting it has. I think it would be good if they started putting them on the...
  11. Replies
    19
    Views
    7,977

    To use the pulse dont you use a different gas...

    To use the pulse dont you use a different gas from the 75/25. Is pulse only used in spray transfer?
  12. Replies
    32
    Views
    16,290

    Thats good he paid you. I too would use a chain...

    Thats good he paid you. I too would use a chain and lock on all items left outside so that doesnt happen again. We have company trailers stole before and thats not something that is good. We...
  13. Replies
    20
    Views
    12,204

    what size of wire are you using.

    what size of wire are you using.
  14. Replies
    20
    Views
    12,204

    They are lookin good. But why are you running it...

    They are lookin good. But why are you running it full speed on 11 ga?
  15. Im in with 301 posts

    Im in with 301 posts
  16. I have some old 7018 3/32 and when I use them...

    I have some old 7018 3/32 and when I use them just throw a hand full in my toaster oven. I too have to lay mine diagnal and if you get too many the door sometimes is hard to close. But they do work...
  17. Replies
    21
    Views
    14,886

    Agreed with 7018 most of the time. Also 6010s....

    Agreed with 7018 most of the time. Also 6010s. Mojority of the rods I use is 7018 becuase they work for thick not to bad for thinner.
  18. Replies
    10
    Views
    6,446

    Its really weird but may be nice. The only bad...

    Its really weird but may be nice. The only bad thing is that it outs every post in section and makes it harder to read them all. Its easy to skip one over when the last one chaged shades when you...
  19. Replies
    15
    Views
    7,876

    Ill try that to see if it works. After it...

    Ill try that to see if it works. After it catching fire once will be a big hesitant.
  20. Replies
    3
    Views
    3,256

    Did it say what this big of a i beam would be...

    Did it say what this big of a i beam would be used for and what size it was. That would be like 100s of pounds of rods.
  21. Replies
    15
    Views
    7,876

    True true. And Ill have a look and see if its...

    True true. And Ill have a look and see if its messed up. Shoot might not even have one in there.
  22. Replies
    51
    Views
    28,215

    on the wheels we have little casters on a welding...

    on the wheels we have little casters on a welding table and it is so hard to push. Get big ones they prolly work better.
  23. Replies
    51
    Views
    28,215

    so how much does everyone usually spend on a top...

    so how much does everyone usually spend on a top for their table. I sure would like having me a good welding table that dont catch on fire and wont warp and as cheap as possible. Prolly 1/4" would be...
  24. Replies
    15
    Views
    7,876

    I might try the rebuild kit. Does the seal in the...

    I might try the rebuild kit. Does the seal in the torch have to be heat resistant? Im seriously thinking about a plasma and just a little *0 cf torch set so its good and portable.
  25. Replies
    15
    Views
    7,876

    well i think I almost have my mind settled with...

    well i think I almost have my mind settled with going plasma. Alot of the stuff I cut is smaller and a plasma will do much better then a torch.
Results 1 to 25 of 321