    Step down to an .045 or even a .035 Dia filler...

    Step down to an .045 or even a .035 Dia filler material. I find when welding stainless tube that 80 amps is a little hot. I use the 1 amp per .001 rule and with stainless 60 amps can be too hot for...
  2. Thank you. Suggested angle? Right now I have...

    Thank you.

    Suggested angle? Right now I have them at 30 degrees with a blunt.
  3. 75 amps Frequency 120hz 30% EP 14006

    75 amps
    Frequency 120hz
    30% EP

    14006
  4. I may have not made my self clear. How would...

    I may have not made my self clear.

    How would you prep a 1/16' dia tungsten for AC welding using no more than 50 - 60 Amps.

    Would you leave it square cut and add amperage to obtain a good...
  5. Number 5 10-12 CFH

    Number 5

    10-12 CFH
  6. Tungsten preparation - Aluminum - 1/16th Dia Eletrode

    As title specifies

    Recommended tungsten prep

    2% EWLa 1/16th Dia.

    Whats crackin? I am new to the forum and made an intro post in the Intro section.

    I am getting back into welding after...
  7. Replies
    0
    Views
    2,305

    255 Ext - New Owner

    Howdy Y'all,

    Name here is Jeb. I am from Texas.

    I got started many moons ago as a welder and graduated to QC/CWI. I currently work work a Metallurgical and Testing lab as the ASME welder...
Results 1 to 7 of 7