I believe that plug is 220v but they might have changed the new ones to 110v. I would use a voltage test on it before plugging any thing in to it.
Type: Posts; User: TheGary
I believe that plug is 220v but they might have changed the new ones to 110v. I would use a voltage test on it before plugging any thing in to it.
I would still get it if I were you. The max inrush is 34amps a 30 amp circuit would probably handle the surge for a couple seconds and that is all you need. If it does pop the breaker all you would...
I do not have a 211I but that is informative. My Thermal arc 250 GTS. would not work with +20 degree temps. It is 2000 vintage so I chalked it up to early stage inverter quirks. This is something...
That says -4 degrees not not below freezing. I understand thet there are temp ranges for electronics but -4 degrees is a lot different than +32 degrees . I can go along with that but not 32 degrees....
This not true. If that was the case half the work in the world would have never been done. If that were the case every manufacturer would have that in their manual .You are the first person in my...
Is this a problem with all the MTS welders? I have an MTS250S and so far have not had this issue. Mine is in an enclosed trailer all the time with no heat and I have not had a problem . I did have...
I talked to Oleg, He is sending out the parts I need for my machine. My machine has been working and I have been using it. It just needed a few parts replaced to make it like new again. Thanks...
I did not want to bother you on a weekend. I will call you monday
I am glad to hear it. I really like Everlast and am glade that it was you that had it deleted. You have restored my confidence in them too. What other company VIP would personally take care of a...
I do not expect Everlast to be perfect and I had a lot of respect for a company that did not delete negative comments and tried to fix things but I have to reassess this now. I was just on a thread...
It has a surge of 33 amps. I would use a 50 amp receptical and use a 40 amp or 50amp breaker. This would allow you to use almost any single phase welder or plasma cutter on the circuit in the future.
I was just wondering why everlast does not make some 220v- 440v welders. These would be much more versatile than 3 phase models. I would say 90% of the industrial welders I have use in my career...
The woosh is because the hose that is used is expanding and when you strike an arc and the gas valve opens the hose is collapsing back to normal size. Go buy a good quality gas hose and replace it....
Thanks for posting . It seams like all you ever hear are the horror stories. Im glade that Everlast took care of you.
Very true.
Well I decided to make an adapter to use my hand plasma torch. If anyone has a Trafimet s-75 hand torch they do not need I would still buy it to keep in the adapter. I probably have enough time in...
Your right, there is not much going on here since the site has been screwed up. Pictures won't post and there are some features like edit that do not work. They are losing a lot of traffic here...
I am looking for a used machine torch to fit my PP60. If anyone has one let me know. Thanks
I see that it does not weld AC stick in the literature now that I am looking for it. I just never saw an AC/DC welder that wouldn't before so it never even entered my head that it wouldn't. I have...
I know for a fact that the pulse control is in the off position. The weld arc seems to fluctuate almost like someone was turning the amp control while I am welding .The weld looks fine but it just...
Ok I have read the on line manual and there is nothing about pulse mode mentioned in stick welding setup instructions. I do not know if that is what is happening . I am just guessing.
Will this machine even do AC stick? When I set it on stick the polarity control does not work. When stick welding It seems to be in DC and I can change polarity by switching ports but nothing tells...
In my experience each welding machine and operator all have different feel and run a rod different. Run it where it works the best for you andthat will be way different when you change to a different...