    It was neither of those. I changed the whole...

    It was neither of those. I changed the whole clunky stock set up out and the wp17 I had was old and was shorting out . I didn't notice until I actually tried a quick weld with an ungloved hand.
  2. Replies
    15
    Views
    9,473

    Actually, it operates exactly like Jody said,...

    Actually, it operates exactly like Jody said, like I had it set, it was a bad torch. I changed the torch and it welded fine. Thanks
  3. Replies
    15
    Views
    9,473

    I picked up some 6011 and that problem is solved....

    I picked up some 6011 and that problem is solved. Now I have issues withe the tig settings. I set it up the way Jody from Tricks and tips showed in a video and all it's doing is burning up tungstens...
  4. Replies
    15
    Views
    9,473

    That's funny because I was using 6010. What...

    That's funny because I was using 6010. What should I use? 6011 , 6013? I did download the manual since I didn't get one with the machine. I'll be the first to admit that I hate technical reads.
  5. Replies
    15
    Views
    9,473

    First of all, In Tig mode, the digital amperage...

    First of all, In Tig mode, the digital amperage values fluctuate even before I weld. They bounce back and forth between two or three values. Yesterday I was trying to weld some 1/8" steel with stick...
  6. Replies
    15
    Views
    9,473

    Power Pro 205s fine tuning

    Does anyone know of any really good videos on how to fine tune the Power Pro 205s. I have the AC tig settings fairly well tuned in but everytime I change over to Stick or DC tig, I have a learning...
  7. Replies
    5
    Views
    3,744

    Thanks for the welcome and the info guys !

    Thanks for the welcome and the info guys !
  8. Replies
    5
    Views
    3,744

    TigFreak- New to the site

    I just set up my new Power Pro 205s and with a little tweaking got it running pretty decent welds. I'm a welding student in my 2nd year of my degree and I gotta say, I love welding ! Particularly...