Search:

Type: Posts; User: performance

Page 1 of 20 1 2 3 4

Search: Search took 0.02 seconds.

  1. Replies
    4
    Views
    90

    Well call tech support at ext 207. The unit has...

    Well call tech support at ext 207. The unit has a 5 year warranty with original bill of sale.
  2. Replies
    1
    Views
    74

    did you call ext 207 or my extension when you...

    did you call ext 207 or my extension when you reached out? I don't have any emails or voice mails about such a machine. Call me.
  3. Replies
    1
    Views
    83

    It can be used for heat control OR for improving...

    It can be used for heat control OR for improving appearance of the weld, depending on the frequency and exact settings you choose. Consider pulse as another tool in your tool box. No one can tell...
  4. Replies
    4
    Views
    90

    Power switch if the display does not light as...

    Power switch if the display does not light as well.
  5. Have you called tech support yet? If you did,...

    Have you called tech support yet? If you did, what did they say? This would be the best way to get this figured out. If you don't have the number, please call 877 755 9353 ext 207.
  6. Replies
    3
    Views
    258

    Seeing the video, it looks like you are an 1 or...

    Seeing the video, it looks like you are an 1 or more away. It definitely is too far off now.
    If you have an extra hand, have someone take a look at the wire feeder while you are welding to see if...
  7. Replies
    4
    Views
    1,850

    Call ext 207 to see what is available.

    Call ext 207 to see what is available.
  8. Replies
    1
    Views
    298

    Call tech support at ext. 207. They can help.

    Call tech support at ext. 207. They can help.
  9. Mostly low end Amps for really thin material, but...

    Mostly low end Amps for really thin material, but not anything significant. But what exactly what features are missing depend upon the model you ultimately select. Most items are small or not as...
  10. Replies
    7
    Views
    744

    Just look around. Bernard has it too....

    Just look around. Bernard has it too.
    https://www.tregaskiss.com/wp-content/uploads/2020/12/SpSh_DirectPlug.pdf
  11. Replies
    7
    Views
    744

    ESAB and Thermal Arc used Euro type for years. ...

    ESAB and Thermal Arc used Euro type for years. So has everyone from Snap on to Clarke.
  12. 60A breaker.

    60A breaker.
  13. Replies
    7
    Views
    744

    Most people with experience I have seen hate the...

    Most people with experience I have seen hate the fusion gun.

    Dozens of manufacturers use and have used the MB15, so yes, there is a huge market. Everyone from Snap On to Clarke has used this gun,...
  14. Don't ball to begin with. What you are...

    Don't ball to begin with. What you are experiencing is nodules. This can do with tungsten contamination from the metal, or with tungsten quality itself, even grinding angle and grind quality. The...
  15. Replies
    7
    Views
    744

    EVERY manufacturer makes a Euro back end for...

    EVERY manufacturer makes a Euro back end for their guns as far as I know. They have to. Miller and Lincoln don't even use their proprietary connections overseas. They use the Euro one on most of...
  16. Replies
    5
    Views
    574

    It does make a difference, but an untrained eye...

    It does make a difference, but an untrained eye may not see it as much, depending upon the wire diameter.
  17. More than likely it is in port. But they are...

    More than likely it is in port. But they are average 90 ships in wait. It's the luck of the draw sometimes who and what gets unloaded first.
  18. These are not offered. But you can call tech...

    These are not offered. But you can call tech support at ext 207 for free help and targeted schematic for your affected part.
  19. That's what I'd do if I wasn't sure.

    That's what I'd do if I wasn't sure.
  20. Welcome. The MTS series does everything quite...

    Welcome. The MTS series does everything quite well. Yes, you need a water cooler with a water-cooled torch. Anything over 200A will require a water cooled torch anyway because the largest air...
  21. Replies
    1
    Views
    542

    Welcome to Everlast.

    Welcome to Everlast.
  22. Replies
    5
    Views
    574

    Have you looked at the manual?

    Have you looked at the manual?
  23. Replies
    1
    Views
    451

    Are you running with the torch in negative for...

    Are you running with the torch in negative for AC? Make sure your work clamp is attached directly to the metal when using other wave forms. Also you may need to check the HF point gap to improve the...
  24. Also don't put your balance above 35%.

    Also don't put your balance above 35%.
  25. No manual. They set up basically like all spool...

    No manual. They set up basically like all spool guns. Simple, straight forward.
Results 1 to 25 of 500