Get the SSC pedal. Well worth the money. I have tried mine on AC and DC and it's just as good as Miller or lincoln units
Type: Posts; User: Datsun1973
Get the SSC pedal. Well worth the money. I have tried mine on AC and DC and it's just as good as Miller or lincoln units
It was the pre flow! Doh! It helps to understand the machine. Works like a champ, crisp starts and stable arc.
Mark, can you please post up the diagnostic procedure for the SSC pedal? I will bust out the ohm meter and check it against specs.
Thanks
I will double check when I get home today and let you know. I know I was in 2t mode.
I have been playing with my new 250ex and been noticing that it takes about 3/4 travel on the pedal before the arc kicks off. I am using 2% lan, 150a, 3/32 tungsten. Is this normal for an inverter...
Got a note from Oleg. CK never shipped the Dinse. Oleg is going to send me a refund and I ordered the connector SL8-35QD from weld fabulous. I also ordered a stubby gas lens kit, cable cover and some...
Emailed Oleg this evening expecting a response tomorrow. Got one within 5 min. Kudos! Not too many companies still exhibit this level of service especially after the sale. I am a sales...
The Welder is here!!! I actually got two packages. One box had the welder and upgraded torch. The other was the pedal from SSC. I am missing the dinse connector. Is this a 3rd package or ??? I...
While I understand the need for PFC on a transformer machine why is it required on these inverters? 60 amps doesn't seem like that much for an input circuit especially when you consider the "welder...
Very cool! My last job was selling M250 engines for Rolls-Royce used in many a Bell Jet Ranger. Before that I was an integration engineer for them so I can tell you there is some serious work to get...
Nice. I wish I had more time for this kind of project. Judging from your screen name I am guessing A&P or pilot?
So I am going to be spending the week at our dallas office and I am wondering if anyone has a recomendation on a LWS up there. I am normally down in Waco and we have several, praxair, airgas and...
That's what I thought on the ck stuff but to my surprise it was there. Mark I will give you a ring when it comes time for the water cooled upgrade. I am hoping I can get up and running next weekend...
Mark while I agree the DV is nice I have my smaller 110v Lincoln Mig for light duty stuff. I sent you an email on the gas lens stuff.
Actually they had the 26 in stock with a 25' super flex cable so that is coming with the welder. I am not sure on the adapter and the pedal but I guess I won't be welding next weekend if that is the...
Anyone know the best place to get a torch parts kit gas lens etc for the 26??
Honestly I asked Oleg about the construction and reliability and he said the 250 was more of a commercial machine. That and it wasn't that much more expensive for the 250. I don't need dual voltage...
So I called today and pulled the trigger on a 250ex with what I call the pro package. CL26 torch and ssc pedal. They even shipped it all today with arrival on the 28th. Off to a good start Everlast.
Thanks Mark. Will do. I was thinking the super flex as well with the 25' option cable.
Yeah I plan to do that. I am hoping the sales folks would use this as an opportunity to chime in.
Hey guys new to the forums and looking to purchase a 200dv in the near future. I would like to know if Everlast offers a pro type package on the 200dv? Specifically I would like the SSC pedal, a...