    It might be one of several issues. Maybe not...

    It might be one of several issues. Maybe not enough argon flow (or it is getting blown away). Dirt/oils on the filler wire. Most likely, IMHO, it could be contaminants being pulled in from the base...
  2. Replies
    56
    Views
    644,436

    I've got one and I like it. For the price (using...

    I've got one and I like it. For the price (using a coupon) I'm satisfied. The only nit and I think it applies to the Nomad too is the cheap plastic cap feet. I busted one in an instant after a CRS...
  3. Replies
    5
    Views
    5,861

    Welcome to another Jim (and EE type too)! ...

    Welcome to another Jim (and EE type too)!

    Looking forward to your stove design as it morphs along. I'd be a customer of a plans set when you are ready.

    My background is in more discrete &...
  4. Replies
    7
    Views
    43,719

    The next test is to see how well it holds a...

    The next test is to see how well it holds a Moscow Mule!
  5. Replies
    7
    Views
    8,985

    I've got a 250EX and have run a separate stranded...

    I've got a 250EX and have run a separate stranded 10 ga ground to a dedicated 8' ground rod. I've also grounded my garage door rails and opener to that same rod with some solid 8ga. For the short...
  6. Replies
    2
    Views
    4,161

    Hi from Centennial Colorado

    Re-starting my welding life after a long break (since high school and living on ranches). Got a new PowerTig 250EX, a very old Lincoln 110v MIG/FCAW and a Harris Oxy/Acet set. Just waiting for my old...
Results 1 to 6 of 8