  1. Sorry, it's been a bit since I followed up on...

    Sorry, it's been a bit since I followed up on this issue. I have since tried 1/8" tungsten (1.5% Lanthanated) and I continue to have the same results. The end of the tungsten never obtains a smooth...
  2. Mark, I appreciate your input. I will try using...

    Mark, I appreciate your input. I will try using 1/8" tungsten for anything above 150 amps and see if that solves the problem.

    Thank you,

    moltenmetal
  3. 210EXT and 325EXT Abnormal Tungsten consumption/erosion with mid/high amperage

    I'm putting this out there to see if anyone else has ever experienced it. Once I started welding more aluminum, and moderately thick aluminum (3/16 - 1/4 plate), I noticed that my 3/32 tungsten would...