Search:

Type: Posts; User: MikeGyver

Search: Search took 0.03 seconds.

  1. Replies
    2
    Views
    5,469

    PT 200DX Gas Solenoid Issue

    After having some hose to barb sealing issues, I took the cover off my machine to change the gas inlet barb on the gas solenoid to a flare style that is interchangable with my other welders (Miller)....
  2. Replies
    25
    Views
    16,064

    Mark, In case there is any confusion, I do not...

    Mark, In case there is any confusion,
    I do not like the way the pulse feature works PERIOD. Foot pedal or not.

    I am disappointed in my purchase which was led to by an advertising error; I would...
  3. Replies
    25
    Views
    16,064

    Mark, like I just said... it's not up to a paying...

    Mark, like I just said... it's not up to a paying customer to scour all sources of information, tally up your error score, and decipher it. When incorrect information is posted (on the main page none...
  4. Replies
    25
    Views
    16,064

    lol... then I've found the source of the...

    lol... then I've found the source of the confusion.

    Here's a screenshot of the 200DX webpage:

    http://i52.tinypic.com/15z2yc5.jpg

    I fell like I've been 'duped' by your advertised...
  5. Replies
    4
    Views
    6,816

    Try to (quickly) develop the puddle on both sides...

    Try to (quickly) develop the puddle on both sides evenly. Put more heat into the thicker/larger part then add filler to it once the puddle develops. Then merge that blob to the other part by adding...
  6. Replies
    25
    Views
    16,064

    I haven't said anything derogatory toward the...

    I haven't said anything derogatory toward the welder (infact I've given it praise). I've just said that I am disappointed with how the pulser works. For what I use it for it simply does not work...