  1. Replies
    8
    Views
    54

    Arc wandering is the arc looking for a circuit...

    Arc wandering is the arc looking for a circuit path. May be due to a bad work clamp, or an improper clamp location or other operator/environmental issue. If the arc is on, it shouldn't be a welder...
  2. Replies
    8
    Views
    54

    AC has never been an issue with an inverter as...

    AC has never been an issue with an inverter as far as I know. NOt in modern times, (last 20 years). But arc starts usually have to do with work clamp location/condition and other settings...not the...
  3. Replies
    8
    Views
    54

    How old is it?

    How old is it?
  4. Replies
    8
    Views
    276

    Sounds like junk to me.

    Sounds like junk to me.
  5. 14 to 104 F operation. Storage at 40 below is...

    14 to 104 F operation. Storage at 40 below is not recommended.
  6. ESAB atom arc is one that comes highly...

    ESAB atom arc is one that comes highly recommended by several that have tried it.
  7. Replies
    5
    Views
    128

    It's fine, it'll be sort of a soft arc.

    It's fine, it'll be sort of a soft arc.
  8. Replies
    5
    Views
    128

    Usually wrought iron does present issues with...

    Usually wrought iron does present issues with welding. It is super high in carbon and having welded it myself, you need to turn up the heat, and focus the heat on the wrought iron (many times it is...
  9. Apologies. A couple of things you should...

    Apologies.

    A couple of things you should keep in mind. Keep the rod buried. Don't take it out of the puddle. Make sure you have the work clamp directly connected to the part being welded.
    ...
  10. Replies
    1
    Views
    87

    If you use the unit like it is designed to be...

    If you use the unit like it is designed to be used (stacked under the 275, directly to it) then nothing will get caught on the cooler fill neck because your work and torch leads stick out further. ...
  11. Replies
    8
    Views
    276

    I don't see why not.

    I don't see why not.
  12. Just one post is sufficient. See my reply to the...

    Just one post is sufficient. See my reply to the other post you made. My thoughts are along trying a different/better brand.
  13. Replies
    5
    Views
    128

    Turn on 6010. But your amps are a bit low. Try...

    Turn on 6010. But your amps are a bit low. Try 80A. What brand rod? Hobart?
  14. Replies
    8
    Views
    276

    Call the manufacturer. Don't rely on "others" to...

    Call the manufacturer. Don't rely on "others" to inform you. We've seen misinformation before on this stuff.
  15. Replies
    8
    Views
    276

    Northern Tool powerhorse line. They have a...

    Northern Tool powerhorse line. They have a 13000w one about that price. Meets the requirements. A lot of the cheaper products say they are but aren't. If it's duromax or champion, be very careful...
  16. Replies
    12
    Views
    2,940

    Call 877 755 9353 ext 207 tomorrow 9 to 5...

    Call 877 755 9353 ext 207 tomorrow 9 to 5 eastern. Don't delay. If it hasn't been 5 years it should be under warranty. If it has it can be fixed for a reasonable price in comparison to purchasing...
  17. Replies
    12
    Views
    2,940

    Make sure you didn't drop your swirl ring out.

    Make sure you didn't drop your swirl ring out.
  18. Replies
    12
    Views
    2,940

    If it has HF start, then you may have a Plasma...

    If it has HF start, then you may have a Plasma inverter problem. Make sure you have the torch on the negative when you cut. Select 2T.
  19. It is likely you have some setting off in the...

    It is likely you have some setting off in the manual setting portion as it still needs to be set with items like Pre/post flow start/end amps etc. And that you are on pedal only, not pedal 2t or...
  20. Replies
    12
    Views
    2,940

    Is it a true old 205 without an s or si?

    Is it a true old 205 without an s or si?
  21. Any machine is as good as that that we have. In...

    Any machine is as good as that that we have. In fact, I'd say the 206pi is not as good as some of the others, especially our powerarc welders. It's ok. But if you want to get him one, get him a...
  22. Get the 24 if you can not the 25. Imho.

    Get the 24 if you can not the 25. Imho.
  23. The early ones had the 15 series. I'd call in and...

    The early ones had the 15 series. I'd call in and order the unit with the gun you want. 15 was typically enough, but still a little light to support the duty cycle of the unit at max. But if it...
  24. Look in the manual. I think they are in there.

    Look in the manual. I think they are in there.
  25. Replies
    4
    Views
    170

    Well as far as the weight. This weighs less than...

    Well as far as the weight. This weighs less than the old Millermatic 211 and the current hobart 211. Many of the components in the machine are plug and play are are customer serviceable. Many...