So, I have been welding on some sheet metal lately its all 14ga steel and have been supplied a Lincoln 140hd with .035 Fluxcore wire and its just not an attractive weld at all. It burns through super...
Type: Posts; User: EvilBunny
So, I have been welding on some sheet metal lately its all 14ga steel and have been supplied a Lincoln 140hd with .035 Fluxcore wire and its just not an attractive weld at all. It burns through super...
What kind of requirements did you have to meet? (Experience wise, and such)
No, it's Fluxcore wirefeed on the containers too windy for tig or even mig outside by the water. Fortunately being in highschool I have 3 whole periods dedicated to welding so I get 3 hours a day to...
Hello, I am a 16 year old welding student looking to learn as much as I can with various welding forums and am planning on buying my own home EverLast Tig welder. I currently do have a job welding ...